[labnetwork] Preferred sputtering target supplier (for TCOs)
Bill Flounders
bill at eecs.berkeley.edu
Thu Aug 11 20:45:42 EDT 2011
Lesker provides high quality targets.
The material you are 'targeting' is finicky.
If you have no evidence of contamination
and no issues with debonding, I would question
process parameters before Lesker's target quality.
Bill Flounders
UC Berkeley
Kevin McPeak wrote:
> Dear labnetwork subscribers,
>
> Do any of you have recommendations for suppliers for sputtering
> targets? I have been using Lesker targets for my PVD75 sputterer. I am
> perfectly happy with their metal targets but haven't had the best of
> luck RF sputtering Al:ZnO films with their 2% Al2O3 / 98% ZnO target
> (copper backed and Indium bonded). My issues may not be related to
> their target at all but I am interested to hear if others on the list
> feel strongly about certain target suppliers, especially for TCO
> materials like Al:ZnO and ITO. Thanks in advance for your input.
>
> Regards,
> Kevin McPeak
>