[labnetwork] N2 grade for blow guns
Leif Johansen
lej at danchip.dtu.dk
Fri Jan 11 15:48:27 EST 2013
Hello Iulian,
Here at DTU Danchip, we are using purified N2 for the guns in fume hoods and wet benches. We have had the same discussion whether it is overkill to do so, since the most of the impurities in our bulk N2 probably stems from water trace. One could argue that the nice clean process N2 becomes dirty the second it leaves the nozzle. However, we have never changed to bulk N2 and most probably will not do so.
Best regards,
Leif
Leif S. Johansen
Head of Operations
DTU Danchip
Technical University of Denmark
Danchip
Ørsteds Plads, Byg. 347
2800 Lyngby
Direct +45 45255713
Mobile +45 25348992
lesjo at danchip.dtu.dk
www.danchip.dtu.dk/
-----Original Message-----
From: labnetwork-bounces at mtl.mit.edu [mailto:labnetwork-bounces at mtl.mit.edu] On Behalf Of Iulian Codreanu
Sent: 11. januar 2013 17:41
To: Fab Network
Subject: [labnetwork] N2 grade for blow guns
Dear Colleagues,
Would it be overkill or a good idea to supply high purity nitrogen (instead of utility nitrogen) to the blow guns located in cleanroom fume hoods?
Thank you for your help.
Iulian
--
iulian Codreanu, Ph.D.
Director of Operations, UD Nanofab
149 Evans Hall
Newark, DE 19716
302-831-2784
_______________________________________________
labnetwork mailing list
labnetwork at mtl.mit.edu
https://www-mtl.mit.edu/mailman/listinfo.cgi/labnetwork
More information about the labnetwork
mailing list