[labnetwork] Looking for XeF2
Miller, Christina S.
csmiller at anl.gov
Wed Dec 10 09:30:16 EST 2014
I got a bottle from Air Products. You have to ask about it.
Suzanne
From: labnetwork-bounces at mtl.mit.edu [mailto:labnetwork-bounces at mtl.mit.edu] On Behalf Of Morrison, Richard H., Jr.
Sent: Wednesday, December 10, 2014 8:11 AM
To: Paolini, Steven; Fab Network (labnetwork at mtl.mit.edu)
Subject: Re: [labnetwork] Looking for XeF2
The material is only available from Pellchem in South Africa, we got the past bottle through Middlesex Gas (Draper supplier of gases).
Rick
From: labnetwork-bounces at mtl.mit.edu<mailto:labnetwork-bounces at mtl.mit.edu> [mailto:labnetwork-bounces at mtl.mit.edu] On Behalf Of Paolini, Steven
Sent: Tuesday, December 09, 2014 5:55 PM
To: Fab Network (labnetwork at mtl.mit.edu<mailto:labnetwork at mtl.mit.edu>)
Subject: [labnetwork] Looking for XeF2
Dear colleagues,
Just recently, my custom made Xenon Difluoride etcher has become popular with many of my users and I found myself in the horrible and embarrassing predicament of running out of etchant. Since this is somewhat of a specialty item, lead times are astronomical. Is there anybody out there that can lend me a sample cylinder? I will replace it with an identical new one. The cylinder is aluminum and is 2" diameter by 10.5" long measured from the bottom to the centerline of the male VCR fitting on the valve. Similar or not so similar cylinders can be fitted, it's just a matter of finding one.
Thank you in advance.
Steve Paolini
Equipment Dood
Harvard University Center for Nanoscale systems
Steve Paolini
Principal Equipment Engineer
Harvard University Center for Nanoscale Systems
617- 496- 9816
spaolini at cns.fas.harvard.edu<mailto:spaolini at cns.fas.harvard.edu>
www.cns.fas.harvard.edu<http://www.cns.fas.harvard.edu>
________________________________
Notice: This email and any attachments may contain proprietary (Draper non-public) and/or export-controlled information of Draper Laboratory. If you are not the intended recipient of this email, please immediately notify the sender by replying to this email and immediately destroy all copies of this email.
________________________________
-------------- next part --------------
An HTML attachment was scrubbed...
URL: <https://mtl.mit.edu/pipermail/labnetwork/attachments/20141210/619e7bfc/attachment.html>
More information about the labnetwork
mailing list