[labnetwork] RTA's
Bob Hamilton
roberthamilton at berkeley.edu
Mon Mar 17 12:41:42 EDT 2014
Re: RTP's
The UC Berkeley Marvell NanoLab has five AllWin21 RTP's. Four of them
are 610's with extended range pyrometry and one is an 810 ERP. We are
pleased with their operation, reliability as well as good support from
AllWin.
Bob Hamilton
--
Robert Hamilton
University of California at Berkeley
Marvell NanoLab
Equipment Eng. Mgr.
Room 520 Sutardja Dai Hall
Berkeley, CA 94720-1754
bob at eecs.berkeley.edu
Phone: 510-809-8600
Mobile: 510-325-7557
e-mail preferred
On 3/17/2014 5:38 AM, Ferraguto, Thomas wrote:
>
> Colleagues
>
> We're looking for a table top RTA. We found *Jipelec Jetfirst 200
> circa 2008* on the used market.
>
> We're a little concerned about an aging operating system (it's
> probably has Windows 95 or 98)
>
> If you have any opinions on the Jipelec unit or any other table top
> you may have an opinion on your input would be welcome.
>
> Best Regards
>
> */P.S> Don't forget to Sign up for UGIM /*
>
> *//*
>
> */http://www.cns.fas.harvard.edu/UGIM2014//*
>
> *//*
>
> Thomas S. Ferraguto
>
> ETIC Nanofabrication Laboratory Director
>
> University of Massachusetts Lowell
>
> 1 University Avenue
>
> Lowell MA 01854-5120
>
> 978-934-1809 land
>
> 617-755-0910 mobile
>
> 978-934-1014 fax
>
>
>
> _______________________________________________
> labnetwork mailing list
> labnetwork at mtl.mit.edu
> https://www-mtl.mit.edu/mailman/listinfo.cgi/labnetwork
--
Robert Hamilton
University of California at Berkeley
Marvell NanoLab
Equipment Eng. Mgr.
Room 520 Sutardja Dai Hall
Berkeley, CA 94720-1754
bob at eecs.berkeley.edu
Phone: 510-809-8600
Mobile: 510-325-7557
e-mail preferred
-------------- next part --------------
An HTML attachment was scrubbed...
URL: <https://mtl.mit.edu/pipermail/labnetwork/attachments/20140317/654de442/attachment.html>
-------------- next part --------------
A non-text attachment was scrubbed...
Name: not available
Type: image/png
Size: 57996 bytes
Desc: not available
URL: <https://mtl.mit.edu/pipermail/labnetwork/attachments/20140317/654de442/attachment.png>
More information about the labnetwork
mailing list