Mason,
Nanostrip I used to buy comes with plastic container. I haven't had any issue in storing for long period of time. I buy from Capitol Scientific (Cyantek(r) KMG Nano-Strip 2X(r)). Sometimes you may need to have different cap on the lid which might remove the buildup pressure from the Nanostrip.
-Shiva
From: labnetwork-bounces at mtl.mit.edu [mailto:labnetwork-bounces at mtl.mit.edu] On Behalf Of Mason Risley
Sent: Wednesday, November 2, 2016 9:17 AM
To: labnetwork at mtl.mit.edu
Subject: [labnetwork] Nanostrip Storage Container
All,
Has anyone experienced problems with storing nanostrip solution (a stabilized form of piranha)? We recently purchased a gallon of it, the first shipment did not arrive due to "damaged packaging during shipment" the second round did in fact arrive but the bottle itself (which is just a plastic HDPE 4L chemical bottle) appears to be degrading, chemical label is completely gone and the plastic lining is - is this something that can be stored in a glass container?  It seems interesting that something specifically engineered and used for dissolving organics and removing polymers is stored in a plastic container.
Thanks,
Mason Risley
Process Development Engineer
Carnegie Mellon University Nanofabrication
5000 Forbes Street, Pittsburgh PA 15213
nanofab-staff at lists.andrew.cmu.edu<mailto:nanofab-staff at lists.andrew.cmu.edu> | http://www.nanofab.ece.cmu.edu/
ph: 412.268.5419 | cell : 505.795.4805
-------------- next part --------------
An HTML attachment was scrubbed...
URL: <https://mtl.mit.edu/pipermail/labnetwork/attachments/20161103/487a9028/attachment.html>
    
    
More information about the labnetwork
mailing list