[labnetwork] Anthracene Evaporation
Mark Heiden
mheiden at engr.ucr.edu
Fri Aug 3 00:29:44 EDT 2018
Does anyone have experience with thermal evaporation of anthracene powder?
We have a request for this material in our thermal evaporator but it is completely foreign to us.