Hi,
I have a question about Chloride in DI water, the E1 water spec states 0.1ppm for Chlorides, have any of your operations monitor for this?
I had a test done and my6 redcir tank is 10ppm and the RO output is 25 these seem high to me, any data out there
Rick
Richard H. Morrison
Principal Member of the Technical Staff
Draper
555 Technology Square
Cambridge, MA
02139-3573
Work 617-258-3420
Cell 508-930-3461
www.draper.com<http://www.draper.com>
________________________________
Notice: This email and any attachments may contain proprietary (Draper non-public) and/or export-controlled information of Draper. If you are not the intended recipient of this email, please immediately notify the sender by replying to this email and immediately destroy all copies of this email.
________________________________
-------------- next part --------------
An HTML attachment was scrubbed...
URL: <https://mtl.mit.edu/pipermail/labnetwork/attachments/20190604/fa00a6e2/attachment.html>
More information about the labnetwork
mailing list