Hi Everyone,
For years we have been using Sensarray wafers to calibrate ovens and hot plates, the issue is they are silicon and break and at $7.5 k each it is costing me $$ I would rather spend on other things.
Do any of you use temperature calibration wafers made of metal, I used to get anodized Aluminum wafers for handler issues from H2Squared are they still around?
Thanks
Rick
Richard H. Morrison
Principal Member of the Technical Staff
Draper
555 Technology Square
Cambridge, MA
02139-3573
Work 617-258-3420
Cell 508-930-3461
www.draper.com<http://www.draper.com>
________________________________
Notice: This email and any attachments may contain proprietary (Draper non-public) and/or export-controlled information of Draper. If you are not the intended recipient of this email, please immediately notify the sender by replying to this email and immediately destroy all copies of this email.
________________________________
-------------- next part --------------
An HTML attachment was scrubbed...
URL: <https://mtl.mit.edu/pipermail/labnetwork/attachments/20190613/68fd79c6/attachment.html>
More information about the labnetwork
mailing list