[labnetwork] Bismuth Telluride thin film deposition
Shimon Eliav
shimonel at savion.huji.ac.il
Sun Nov 24 10:12:26 EST 2019
I would not perform this on an evaporator: Bi, Te and Bi2Te3 all have relatively high vapor pressure at relative low temperature.
Shimon
From: labnetwork-bounces at mtl.mit.edu [mailto:labnetwork-bounces at mtl.mit.edu] On Behalf Of Bill Kiether
Sent: Friday, 22 November 2019 17:10
To: labnetwork at mtl.mit.edu
Cc: Philip Barletta <pbarlet at ncsu.edu>
Subject: [labnetwork] Bismuth Telluride thin film deposition
Hello,
Does anyone offer bismuth telluride PV deposition (evap or sputter) as a service, or have experience with it from a safety and tool perspective?
We have a need for depositions of 300 nm-2um bt on 4" oxide-on-silicon wafers, and want to explore all the options.
Bill Kiether, PhD
Photonics Lab Manager, NCSU
wjkiethe at ncsu.edu<mailto:wjkiethe at ncsu.edu>
-------------- next part --------------
An HTML attachment was scrubbed...
URL: <https://mtl.mit.edu/pipermail/labnetwork/attachments/20191124/12323fe8/attachment.html>
More information about the labnetwork
mailing list