[labnetwork] Diffusion ZnO on InAs in forming gas

Beaudoin, Mario beaudoin at physics.ubc.ca
Tue Aug 30 19:22:12 EDT 2022


I never allow Zn containing materials to be deposited in any of my 
chambers.  Exactly for that reason.

Mario

On 2022-08-30 2:13 p.m., Brian K. Olmsted wrote:
> [*CAUTION:* Non-UBC Email]
>
> Hi Paul,
>
> Others may want to add to this with their experiences, but I have used 
> ZnO in a retort furnace using a forming gas environment and the net 
> result was Zn contamination so bad and persistent that the furnace was 
> decommissioned and could not be used anymore.
>
> Thanks,
>
> Brian
>
> On Tue, Aug 30, 2022 at 2:36 PM Steffen, Paul <steffen.8 at osu.edu> wrote:
>
>     Lab Network Community,
>
>     We have a request to diffuse ZnO on InAs in forming gas at 450 C
>     for 1 hour in a horizontal furnace tube. Does anyone have
>     experience with these materials in forming gas? Would the forming
>     gas react with either material leading to decomposition and
>     contamination of the furnace tube with Zn or As?
>
>     Thanks.
>
>     -Paul
>
>     The Ohio State University
>     *Paul Steffen*
>     Lab Manager
>     Institute for Materials ResearchNanotech West Lab
>     100 Science Village, 1381 Kinnear Road, Columbus, OH 43212
>     614-688-3546 Office / 614-688-3379 Fax
>     steffen.8 at osu.edu <mailto:steffen.8 at osu.edu>nanotech.osu.edu
>     <http://nanotech.osu.edu>
>
>     _______________________________________________
>     labnetwork mailing list
>     labnetwork at mtl.mit.edu
>     https://mtl.mit.edu/mailman/listinfo.cgi/labnetwork
>
>
> _______________________________________________
> labnetwork mailing list
> labnetwork at mtl.mit.edu
> https://mtl.mit.edu/mailman/listinfo.cgi/labnetwork
-- 
-------------- next part --------------
An HTML attachment was scrubbed...
URL: <https://mtl.mit.edu/pipermail/labnetwork/attachments/20220830/a0249cc7/attachment.html>
-------------- next part --------------
A non-text attachment was scrubbed...
Name: image001.png
Type: image/png
Size: 3605 bytes
Desc: not available
URL: <https://mtl.mit.edu/pipermail/labnetwork/attachments/20220830/a0249cc7/attachment.png>
-------------- next part --------------
A non-text attachment was scrubbed...
Name: Mario%20Beaudoin%20SBQMI%20sig%202.jpg
Type: image/jpeg
Size: 21446 bytes
Desc: not available
URL: <https://mtl.mit.edu/pipermail/labnetwork/attachments/20220830/a0249cc7/attachment.jpg>