[labnetwork] CDA and copper piping
Collins, Deon
deonc69 at illinois.edu
Thu Dec 8 10:46:21 EST 2022
Our entire system is copper. There are standards depending on your needs. You should be using type L copper for Med Gas. Silver soldered joints are a preferred method for Med Gas. The compressor, dehumidifier and filters play as large a role as the materials.
From: labnetwork <labnetwork-bounces at mtl.mit.edu> On Behalf Of Denis, Kevin L. (GSFC-5530)
Sent: Wednesday, December 7, 2022 3:46 PM
To: labnetwork at mtl.mit.edu
Subject: [labnetwork] CDA and copper piping
Hello All,
Has anyone used copper piping for clean dry air lines. If not what kind of problems would one run into if going this route? Thanks for any insight that can be provided.
Regards,
Kevin