[labnetwork] Question about DC sputtering of zinc
Shawn Wagoner
swagone at gmu.edu
Wed Feb 1 07:22:52 EST 2023
I would not allow Zinc in any system I ran at Binghamton University. I would not even allow it in the cleanroom. It represents a significant contamination risk for shared use facilities. If I were fortunate enough to have two systems, one clean and one "dirty", I might consider it in the dirty system. Its vapor pressure is so high I am not sure there is much you can do to cover it up with Ti.
Shawn
From: labnetwork <labnetwork-bounces at mtl.mit.edu> On Behalf Of Malhotra, Sandra Guy
Sent: Monday, January 30, 2023 4:40 PM
To: Fab Network <labnetwork at mtl.mit.edu>
Subject: [labnetwork] Question about DC sputtering of zinc
Howdy All from AggieFab,
We have a user who requested permission to sputter zinc in our shared Lesker PVD75 DC sputtering tool. On the Lesker website, there is the following note:
"This material has a relatively high vapor pressure at low temperatures which can cause ppm level contamination in the chamber and subsequent films. Careful consideration should be taken before this material is used in any deposition system. For this reason, some users prefer to use only dedicated vacuum chambers for deposition."
I'd like to ask the group if they allow zinc depositions in their shared tools if they follow it by a thorough paste with another material, like Ti? Or if this material is prohibited because it is problematic.
Thanks in advance for any inputs you may have.
Best,
Sandra G. Malhotra, Ph.D. | Technical Lab Manager
AggieFab Nanofabrication Facility
https://aggiefab.tamu.edu/<https://nam11.safelinks.protection.outlook.com/?url=https%3A%2F%2Faggiefab.tamu.edu%2F&data=05%7C01%7Cswagone%40gmu.edu%7C701883f7c7244957be4108db03237a96%7C9e857255df574c47a0c00546460380cb%7C0%7C0%7C638107223189605602%7CUnknown%7CTWFpbGZsb3d8eyJWIjoiMC4wLjAwMDAiLCJQIjoiV2luMzIiLCJBTiI6Ik1haWwiLCJXVCI6Mn0%3D%7C2000%7C%7C%7C&sdata=Qvwl9IyHCzbpDHi%2BTs1FZrY65j79ftUQV83kJBELqLg%3D&reserved=0>
Department of Electrical & Computer Engineering, College of Engineering | Texas A&M University
3253 TAMU | College Station, TX 77843
ph: 979.845.3199 | sandra.malhotra at tamu.edu<mailto:sandra.malhotra at tamu.edu>
- - - - - - - - - - - - - - - - - - - - - - - -
TEXAS A&M UNIVERSITY | FEARLESS on Every Front
-------------- next part --------------
An HTML attachment was scrubbed...
URL: <https://mtl.mit.edu/pipermail/labnetwork/attachments/20230201/93854a63/attachment.html>
More information about the labnetwork
mailing list