[labnetwork] PDMS processing - separate lab?

Sandrine Martin sandrine at umich.edu
Wed Sep 4 16:59:46 EDT 2024


Hello Dan,

At U Michigan, we started many years ago with PDMS in the cleanroom and
soon moved it to our separate, quasi-class 10,000 lab space where we now
have a dedicated bay for soft lithography and similar processes.

Thanks
Sandrine

On Wed, Sep 4, 2024 at 3:12 PM Dan P. Woodie <daniel.woodie at princeton.edu>
wrote:

> Lab Network,
>
>
>
> I am curious how many fabs allow PDMS mixing in their main cleanrooms and
> how many require that work done in separate isolated spaces or noncleanroom
> labs. My experience has been that they can be in the same space if careful
> glove protocols are used to avoid spreading the unpolymerized precursors
> around the facility, but I am interested in other’s experiences. Thanks for
> the shared knowledge.
>
>
>
> Dan
>
>
>
> Daniel Woodie
>
> Director, Micro/Nano Fabrication Center, Princeton Materials Institute
>
> Princeton University
>
> 155 Andlinger Center
>
> 86 Olden St
>
> Princeton, NJ 08540
>
>
>
> (609)258-5922 (office)
>
> (607)227-2993 (cell)
>
> daniel.woodie at princeton.edu
>
> mnfc.princeton.edu
>
> www.linkedin.com/in/danielpwoodie
>
>
>
>
>
>
>
>
> _______________________________________________
> labnetwork mailing list
> labnetwork at mtl.mit.edu
> https://mtl.mit.edu/mailman/listinfo.cgi/labnetwork
>


-- 

Sandrine Martin, Ph.D. (she/her/hers)

University of Michigan

LNF Managing Director

1246D EECS, 1301 Beal Ave

Ann Arbor, MI 48109

Cell 734-277-2365

www.LNF.engin.umich.edu <http://www.lnf.engin.umich.edu/>

@LurieNanofab
-------------- next part --------------
An HTML attachment was scrubbed...
URL: <https://mtl.mit.edu/pipermail/labnetwork/attachments/20240904/0a018416/attachment.html>


More information about the labnetwork mailing list