Hi Gohmyeong,
   Quality bonds are going to be very sensitive to particles.  We have our bonder in the class 100 (yellow) area.

-Michael
________________________________
From: labnetwork <labnetwork-bounces at mtl.mit.edu> on behalf of Gohmyeong Bae <gohmyeongbae at umass.edu>
Sent: Wednesday, April 23, 2025 5:57 PM
To: labnetwork at mtl.mit.edu <labnetwork at mtl.mit.edu>
Subject: [labnetwork] SB6 substrate bonder at white room?


CAUTION: This email originated from outside of our organization. Do not click links, open attachments, or respond unless you recognize the sender's email address and know the contents are safe.

Dear Labnetwork,

We had concerns about putting our SB6 substrate bonder into the white or yellow area.

I had seen these types of tools in white room, but should it be necessary need for yellow area for all applications?

Thank you.

Get Outlook for Android<https://aka.ms/AAb9ysg>
-------------- next part --------------
An HTML attachment was scrubbed...
URL: <https://mtl.mit.edu/pipermail/labnetwork/attachments/20250424/e087960d/attachment.html>


More information about the labnetwork mailing list