Travis,
Good morning. Here at UofMichigan, we were using a pressure booster (see
attached photo) for a nano-imprinter application where we needed 1500PSI
N2. This worked ok, and we used a cylinder as the storage tank so that we
had some volume. However after having to rebuild this pressure builder
unit twice in the span of 12 months (bad seals), it became easier to just
use a cylinder of N2 gas, and swap the cylinders out as needed.
Haskel makes some good stuff, when I was looking to do 15,000PSI Helium
testing, but I've never actually worked with any of their equipment.
Thanks,
Dennis Schweiger
University of Michigan/LNF
Facilities
734.647.2055 Ofc
On Wed, Aug 6, 2025 at 11:40 AM Travis Venables <venables at seas.upenn.edu>
wrote:
> Hello everyone,
>
> Here at QNF we have a need to bring our house N2 pressure (sitting at
> 100psi) up to 500-750psi for a Nanonex NX2600 Nanoimprint tool. We
> currently utilize a Maximator system which is controlled pneumatically with
> house CDA. We are having a lot of issues with o-rings drying up and needing
> regular regreasing which becomes labor intensive. I am curious what
> everyone uses for N2 pressure builders in their facilities. Thanks!
> --
> Travis Venables
>
> Lead Cleanroom Equipment Engineer
> Quattrone Nanofabrication Facility
> University of Pennsylvania
> https://www.nano.upenn.edu
> P: 215-898-1787
>
> _______________________________________________
> labnetwork mailing list
> labnetwork at mtl.mit.edu
> https://mtl.mit.edu/mailman/listinfo.cgi/labnetwork
>
-------------- next part --------------
An HTML attachment was scrubbed...
URL: <https://mtl.mit.edu/pipermail/labnetwork/attachments/20250807/bbe5e450/attachment.html>
-------------- next part --------------
A non-text attachment was scrubbed...
Name: booster pump.jpg
Type: image/jpeg
Size: 195961 bytes
Desc: not available
URL: <https://mtl.mit.edu/pipermail/labnetwork/attachments/20250807/bbe5e450/attachment.jpg>
More information about the labnetwork
mailing list