Dear Jayer,

Our lab has been purchasing masks from Advance Reproductions Corp, and we are pleased with them. Their website is:

http://www.advancerepro.com/.

The emails to their customer service representatives are:

d.robinson at advancerepro.com and m.nadeem at advancerepro.com.

The phone number is:

(978) 685-2991

They are located in Andover, Massachusetts.

A 4 X 4 X 0.090 soda lime coated with chrome cost us $450. This is pricey compared to writing one yourself on the DWL with a blank mask plate, yet it is worth it for us because the improved results are evident in our devices.


  *
The specs they can achieve are 0.75 um for the smallest dimension
  *
The critical dimension tolerance is +/-0.15 um.
  *   Glass sizes range from 3″ to 32″
  *
Substrate materials: quartz, fused silica, soda lime, borosilicate.
  *   Glass coatings: chrome, iron oxide, aluminum, titanium, gold, and emulsion
  *   Plate thickness: .020″ to .400″ (10mm)

I hope this helps you and the rest of the labnetwork community.

Very Respectfully,
Oles
________________________________
From: labnetwork <labnetwork-bounces at mtl.mit.edu> on behalf of Thomas Daunais <tdaunais at hawksemiconductor.com>
Sent: Tuesday, March 4, 2025 7:49 PM
To: Prashant Srinivasan <prashant at ucsb.edu>
Cc: labnetwork at mtl.mit.edu <labnetwork at mtl.mit.edu>
Subject: Re: [labnetwork] Photomask Manufacturing Companies

Jim at Photomask Portal has done exceptional work for us for many years. I couldn't recommend him enough after many other vendors have let us down.
PHOTOMASK PORTAL - We Help You Make Masks<https://www.photomaskportal.com/>


On Tue, Mar 4, 2025 at 7:46 PM Prashant Srinivasan <prashant at ucsb.edu<mailto:prashant at ucsb.edu>> wrote:
I can answer part of your question. We buy mask plates from Nanofilm for  $20 - $25 /ea for 3"-5" sq Soda Lime plates. The masks are written in-house on a Heidelberg DWL 200.
https://www.nanofilm.com/

On 3/4/2025 9:47 AM, JAYER A FERNANDES wrote:
Hi,

I'm curious to know what service/company folks are using to make standard photomasks?

Regards



Jayer Fernandes

Micro/Nano Sensors and Actuators Laboratory (MNSA)
Department of Electrical and Computer Engineering
University of Wisconsin - Madison



_______________________________________________
labnetwork mailing list
labnetwork at mtl.mit.edu<mailto:labnetwork at mtl.mit.edu>
https://mtl.mit.edu/mailman/listinfo.cgi/labnetwork



--
Prashant Srinivasan
Teaching Cleanroom Engineer
Electrical & Computer Engineering
University of California, Santa Barbara
Santa Barbara, California 93106
https://www.ece.ucsb.edu/department-resources/electronics-shop/tcr

_______________________________________________
labnetwork mailing list
labnetwork at mtl.mit.edu<mailto:labnetwork at mtl.mit.edu>
https://mtl.mit.edu/mailman/listinfo.cgi/labnetwork


--
Thomas Daunais, PhD
Lead process engineer
Hawk Semiconductor LLC
300 W. Michigan Ave.
VC-2
Ypsilanti, MI 48197
hawksemiconductor.com<http://hawksemiconductor.com/>
Ph: (231) 740-2720
-------------- next part --------------
An HTML attachment was scrubbed...
URL: <https://mtl.mit.edu/pipermail/labnetwork/attachments/20250305/6d100e15/attachment.html>


More information about the labnetwork mailing list