[labnetwork] Anti-seize coatings for VCR threads

Travis Wade travis at evolvediamonds.com
Wed Mar 12 20:23:13 EDT 2025


Hi Dan,

I've had good luck with Loctite 37617, silver-based antisieze.

https://www.amazon.com/Loctite-37617-6PK-Silver-Grade-Anti-Seize-Lubricant/dp/B0053ZS1Z8?th=1

I only use it on non-vacuum wetted surfaces, typically conflat flange
bolts, so I cannot comment on outgassing, but I would have no aversion to
applying it to a VCR thread.  The glue-stick style applicator is
wonderfully convenient.

Good luck!

Travis Wade, Ph.D.
Evolve Diamonds LLC
Ph. +1 (978) 434-2283


On Wed, Mar 12, 2025 at 3:45 PM Dan P. Woodie <daniel.woodie at princeton.edu>
wrote:

> Most Excellent Lab Network Community,
>
>
>
> We have parts for our ALD tool that returned from cleaning with the silver
> anti-galling layer on the VCR nuts severely damaged. The concern is that
> these are the heated lines that feed the ALD chamber and therefore, after
> being tightened for 6+ months before the next cleaning, the heated
> stainless-steel surfaces will seize up and we won’t be able to remove the
> nut. Is anyone aware of an anti-seize coating or similar options that we
> can apply to these threads to be able to use this damaged manifold? Given
> that the VCR threads are not in the flow path, we are hoping to be able to
> continue use the manifold, as it is quite expensive to replace.
>
>
>
> Thanks for any advice the community can share.
>
>
>
> Dan
>
>
>
> Daniel Woodie
>
> Director, Micro/Nano Fabrication Center, Princeton Materials Institute
>
> Princeton University
>
> 155 Andlinger Center
>
> 86 Olden St
>
> Princeton, NJ 08540
>
>
>
> (609)258-5922 (office)
>
> (607)227-2993 (cell)
>
> daniel.woodie at princeton.edu
>
> mnfc.princeton.edu
>
> www.linkedin.com/in/danielpwoodie
>
>
>
>
>
>
>
>
> _______________________________________________
> labnetwork mailing list
> labnetwork at mtl.mit.edu
> https://mtl.mit.edu/mailman/listinfo.cgi/labnetwork
>
-------------- next part --------------
An HTML attachment was scrubbed...
URL: <https://mtl.mit.edu/pipermail/labnetwork/attachments/20250312/76c28956/attachment.html>


More information about the labnetwork mailing list