Following up on the wet etching theme, piranha solution attacks a lot of
metals, but not Au.

Can you use EDS to determine the other elements?

Robert Nidetz, PhD (he/him/his)
University of Michigan
LNF User Liaison and Domain Expert
1241 EECS Building
1301 Beal Ave
Ann Arbor, MI 48109
nidetz at umich.edu
734.496.8065
Book an appointment: https://calendly.com/nidetz


On Sat, May 10, 2025 at 8:18 AM Czwakiel, James <czwakj at rpi.edu> wrote:

> Dr Rao
>
> We have used scrubbing pads to clean off any oxidation or contamination
> You can also flip it over
> Try the other side
>
> Jim
> RPI
>
>
> Get Outlook for iOS <https://aka.ms/o0ukef>
> ------------------------------
> *From:* labnetwork <labnetwork-bounces at mtl.mit.edu> on behalf of Fubo Rao
> <furao at ucsd.edu>
> *Sent:* Friday, May 9, 2025 6:53:10 PM
> *To:* labnetwork at mtl.mit.edu <labnetwork at mtl.mit.edu>
> *Subject:* [EXTERNAL][labnetwork] ideas to clean gold sputter target
>
>
> *CAUTION:* This email originated from outside of the organization. Do not
> click links or open attachments unless you recognize the sender and know
> the content is safe.
> Dear Colleagues,
>
> What would you recommend for cleaning this Au sputter target that has been
> partially coated/contaminated with other materials? There are probably a
> few material coatings on the target, before this was found out. Sputtering
> the materials off, or sand blasting will waste a lot of gold. Thanks in
> advance.
>
> [image: image.png]
>
> Thanks,
>
> Fubo Rao, Ph.D.,
> Nano3 Technical Director,
> Qualcomm Institute/Atkinson Hall,
> UC San Diego
> <https://www.google.com/maps/search/San+Diego+%0D%0A9500+Gilman+Drive+%230436+%0D%0ALa+Jolla,+CA+92093-0436?entry=gmail&source=g>
> 9500 Gilman Drive #0436
> <https://www.google.com/maps/search/San+Diego+%0D%0A9500+Gilman+Drive+%230436+%0D%0ALa+Jolla,+CA+92093-0436?entry=gmail&source=g>
> La Jolla, CA 92093-0436
> <https://www.google.com/maps/search/San+Diego+%0D%0A9500+Gilman+Drive+%230436+%0D%0ALa+Jolla,+CA+92093-0436?entry=gmail&source=g>
> Tel. (858)534-4518
> Cell: (858)375-9190
> E-mail: furao at ucsd.edu
> https://nanofab.ucsd.edu/
> About Nano3 <https://nanofab.ucsd.edu/about/>
> [image:
> https://www.linkedin.com/company/ucsd-nano3-shared-research-facility/]
> <https://www.linkedin.com/company/ucsd-nano3-shared-research-facility/>
> _______________________________________________
> labnetwork mailing list
> labnetwork at mtl.mit.edu
> https://mtl.mit.edu/mailman/listinfo.cgi/labnetwork
>
-------------- next part --------------
An HTML attachment was scrubbed...
URL: <https://mtl.mit.edu/pipermail/labnetwork/attachments/20250510/de2ac7ff/attachment.html>
-------------- next part --------------
A non-text attachment was scrubbed...
Name: image.png
Type: image/png
Size: 263086 bytes
Desc: not available
URL: <https://mtl.mit.edu/pipermail/labnetwork/attachments/20250510/de2ac7ff/attachment.png>


More information about the labnetwork mailing list