Yeah, don't buy it.  Just make it as needed and keep a close eye on the students.  These days we only really use it to clean stubborn debris on masks and a few other relatively small volume applications. That said, we do have an acid waste neutralization system.

-Michael

________________________________
From: labnetwork <labnetwork-bounces at mtl.mit.edu> on behalf of Prashant Srinivasan <prashant at ucsb.edu>
Sent: Monday, November 17, 2025 8:39 PM
To: Beaudoin, Mario <beaudoin at physics.ubc.ca>; labnetwork at mtl.mit.edu <labnetwork at mtl.mit.edu>
Subject: Re: [labnetwork] Nanostrip/Purestrip bottle leakage: what do most labs do?


CAUTION: This email originated from outside of our organization. Do not click links, open attachments, or respond unless you recognize the sender's email address and know the contents are safe.

Mario,

Is there a particular reason you absolutely need Piranha? I made the switch to RCA in our teaching cleanroom after getting tired of cleaning up spills. Even a few drops burn leave burn marks. RCA is fairly dilute (5:1/6:1) and the use temperature is only 70 C. Also, adding peroxide isn't as fraught. No matter how "well trained" the students are, the Piranha preparation process is unforgiving. Hazards to users, chemical waste and disposal risk (I don't have neutralization capabilities) drove my decision making.

Prashant


On 11/17/2025 10:48 AM, Beaudoin, Mario wrote:

Dear Labnetwork,

As many labs do, because of safety concerns for the students, I banned the use the real pirahna etch in favor of Purestrip (Transene version of nanostrip).  The problem I have is that the solution eventually leaks from the bottle.  I have heard of others mentioning this also.

I am now thinking of revising this policy and going back to old pirahna, despite the issues with safety and aging H2O2.

Anyone have comments?

Mario

--
[cid:part1.3RNpK0vD.7A01NJAU at ucsb.edu]


_______________________________________________
labnetwork mailing list
labnetwork at mtl.mit.edu<mailto:labnetwork at mtl.mit.edu>
https://mtl.mit.edu/mailman/listinfo.cgi/labnetwork


--
Prashant Srinivasan,
Teaching Cleanroom Engineer
Electrical & Computer Engineering
University of California, Santa Barbara
Santa Barbara, California 93106
https://www.ece.ucsb.edu/department-resources/electronics-shop/tcr
-------------- next part --------------
An HTML attachment was scrubbed...
URL: <https://mtl.mit.edu/pipermail/labnetwork/attachments/20251118/3cb07115/attachment.html>
-------------- next part --------------
A non-text attachment was scrubbed...
Name: Mario Beaudoin SBQMI sig 3.jpg
Type: image/jpeg
Size: 22413 bytes
Desc: Mario Beaudoin SBQMI sig 3.jpg
URL: <https://mtl.mit.edu/pipermail/labnetwork/attachments/20251118/3cb07115/attachment.jpg>


More information about the labnetwork mailing list