[labnetwork] FOTS or other SAM coating as a service

Demis D. John demis at ucsb.edu
Sun Oct 26 17:21:23 EDT 2025


We have FDTS in case that’s a useful option for you as well.

-- Demis (contact info <https://wiki.nanotech.ucsb.edu/wiki/Demis_D._John>)
*Reminder*: The NanoFab has a publications policy
<https://wiki.nanotech.ucsb.edu/wiki/Frequently_Asked_Questions#Publications_acknowledging_the_Nanofab>


On Fri, Oct 24, 2025 at 22:10 John Tamelier <jtamelier at ucsd.edu> wrote:

> Hello Sam,
>
> We have the ability to vapor deposit FOTS as a service. Please contact me
> directly for more information.
>
> Best,
>
> John
>
> -----------------------------------
> John Tamelier, Ph.D.
> Assistant Director - Nano3
>
> University of California, San Diego
> Atkinson Hall, 5th Floor Front Desk, M/C 0436
> 3195 Voigt Drive
> <https://www.google.com/maps/search/3195+Voigt+Drive+%0D%0A++++++La+Jolla,+California+92093-0436?entry=gmail&source=g>
> La Jolla, California 92093-0436
> <https://www.google.com/maps/search/3195+Voigt+Drive+%0D%0A++++++La+Jolla,+California+92093-0436?entry=gmail&source=g>
> Phone: (858) 246-2735
> Fax:   (858) 534-9092
> E-mail: jtamelier at ucsd.edu
> https://nanofab.ucsd.edu/
> ----------------------------------
> On 10/23/2025 10:21 AM, Sam Tsitrin wrote:
>
> Colleagues,
> Our MVD100 anti-stiction coating tool is down, is there anyone that does a
> vapor FOTS or other SAM  coating as a service? Thanks.
>
>
> --
> Sam Tsitrin
>
> R&D Engineer
> UC Berkeley Marvell Nanolab
>
> _______________________________________________
> labnetwork mailing listlabnetwork at mtl.mit.eduhttps://urldefense.com/v3/__https://mtl.mit.edu/mailman/listinfo.cgi/labnetwork__;!!Mih3wA!EjsSfCk1bfJ9Ox4IxyxwhK6h0R3XIiOVwbR54O_IUVi7ogKEpFdMYDnBEs_0Z4X1y-krFB8N-3XmjHNv-JnYS2Dolw$
>
> _______________________________________________
> labnetwork mailing list
> labnetwork at mtl.mit.edu
> https://mtl.mit.edu/mailman/listinfo.cgi/labnetwork
>
-------------- next part --------------
An HTML attachment was scrubbed...
URL: <https://mtl.mit.edu/pipermail/labnetwork/attachments/20251026/a1c26dda/attachment.html>


More information about the labnetwork mailing list