Hi Russ,

 

We make PDMS molds in our lab but we have banned it from the cleanroom. It
tends to stick everywhere and since it's transparent, you often don't notice
it until it's too late. We have had pieces sticking on the bottom of wafers.

So now the molds are made outside the cleanroom inside a laminar flow hood.

 

Melhores Cumprimentos/ Best Regards

 

Virginia Soares

 

INESC-MN

Rua Alves Redol,9

1000-029 LISBON

PORTUGAL

Tel: +3513100237

https://inesc-mn.pt

 

From: labnetwork <labnetwork-bounces at mtl.mit.edu> On Behalf Of Russ Renzas
Sent: 4 de setembro de 2025 01:22
To: Lab Network (labnetwork at mtl.mit.edu) <labnetwork at mtl.mit.edu>
Subject: [labnetwork] PDMS mold process?

 

Is anyone familiar with PDMS (or other material) mold fabrication? Any
procedures or gotchas to worry about? 

 

Bio faculty member asking if we can make molds in our fab. I only know how
to make semiconductor, photonic, and quantum devices. 

 

Thanks!

 

Russ

 

Russ Renzas

University of Nevada, Reno

-------------- next part --------------
An HTML attachment was scrubbed...
URL: <https://mtl.mit.edu/pipermail/labnetwork/attachments/20250904/cf022f78/attachment.html>
-------------- next part --------------
A non-text attachment was scrubbed...
Name: image001.png
Type: image/png
Size: 1750 bytes
Desc: not available
URL: <https://mtl.mit.edu/pipermail/labnetwork/attachments/20250904/cf022f78/attachment.png>


More information about the labnetwork mailing list