Hello All,

I'm curious to know what the EMO's do on the wet benches in your
facilities. Do they shut down CDA, N2 or water, or just high voltage? What
is the thought process behind what does/does not get shut down? We recently
had a bad DI water leak on one of our benches, and we were a little
surprised to find out that the EMO did not shut off the water supply, so we
are considering whether or not we want to make a changes to the way the
EMO's work on our benches.

I look forward to reading your replies.

Best,
-- 
Kyle Keenan

Senior Manager - Laboratory Operations
Quattrone Nanofabrication Facility
University of Pennsylvania
P: 215-898-7560
F: 215-573-4925