[labnetwork] PCB in e-beam evaporator?

Russ Renzas rrenzas at unr.edu
Wed Jul 1 22:10:34 EDT 2026


For a summer lab class we're trying to have students make a chip and wirebond it to a PCB. We're having trouble wirebonding to the immersion gold pads though.

Is it okay to put pcbs in our ebeam evaporator to evaporate Au?

We tried a small piece in a Au SEM prep sputter coater and that worked but it's too small for the class PCBs.

Thanks, also appreciate any tips on how to spec pcb metalization for wirebonding compatibility. We have both Al ultrasonic wedge and Au ball bond capabilities.

Russ Renzas
University of Nevada, Reno
-------------- next part --------------
An HTML attachment was scrubbed...
URL: <https://mtl.mit.edu/pipermail/labnetwork/attachments/20260702/055f9d67/attachment.html>