[labnetwork] Cleanroom Particle Monitors
Paul.Weitnauer at sonydadc.com
Paul.Weitnauer at sonydadc.com
Tue May 12 06:31:10 EDT 2026
Hi all,
We’re using the same very cheap particle sensors<https://urldefense.com/v3/__https:/www.adafruit.com/product/4632__;!!O7_YSHcmd9jp3hj_4dEAcyQ!wquIoT7fitQJgL8WUUvYpQTUhW1WS3eJSY737geH720YLE57qXyReEyjj8ccctWXj9HiQqW49mLmDTB_tXn9CLmnlQ$> inspired by luftdaten.info – Feinstaub selber messen – Open Data und Citizen Science aus Stuttgart<https://luftdaten.info/> in combination with offline measurements using a portable calibrated Particle Monitor.
Monitoring is done via Raspberry Pi + InfluxDB + Grafana. Very useful combination for tracking other environmental variables, CA pressure, …
Best regards,
Paul
Paul Weitnauer | Manager Mastering Engineering |
Sony DADC Europe GmbH | Sonystrasse 4 | 5303 Thalgau, Salzburg | Austria
Phone: +43 6246 880 8567 | mobile: + 43 664 82 53 165 | paul.weitnauer at sonydadc.com
www.sonydadc.com<http://www.sonydadc.com/> | Registered Company Number: 542948 | Registered Company: Sony DADC Europe GmbH, Sonystrasse 4, 5303 Thalgau, Austria
[cid:image001.png at 01DCE20B.35E267A0]
For more information on Sony being named one of the 2026 World’s Most Ethical Companies, please click here<https://www.sony.com/en/SonyInfo/News/Press/202603/26-005E/>.
Von: labnetwork <labnetwork-bounces at mtl.mit.edu> Im Auftrag von Sergi Lendinez
Gesendet: Mittwoch, 25. März 2026 16:03
An: Network Fab <labnetwork at mtl.mit.edu>
Betreff: Re: [labnetwork] Cleanroom Particle Monitors
We have very cheap particle sensors<https://urldefense.com/v3/__https:/www.adafruit.com/product/4632__;!!O7_YSHcmd9jp3hj_4dEAcyQ!wquIoT7fitQJgL8WUUvYpQTUhW1WS3eJSY737geH720YLE57qXyReEyjj8ccctWXj9HiQqW49mLmDTB_tXn9CLmnlQ$> to monitor unusual high particle values via NEMO. They are good enough at detecting malfunctioning ACH or deteriorated filters at a fraction of the cost of other particle monitors. I wouldn't use them to know if the spaces meet certification or to know actual particle counts, but they are good to detect anomalies quickly.
Regards,
Sergi
________________________________
From: labnetwork <labnetwork-bounces at mtl.mit.edu> on behalf of Nicholas Menounos <menounos at mit.edu>
Sent: Tuesday, March 24, 2026 5:50 PM
To: Carroll, David <carroldl at wfu.edu>; Nathan Aultman <naultman at creol.ucf.edu>
Cc: Network Fab <labnetwork at mtl.mit.edu>
Subject: Re: [labnetwork] Cleanroom Particle Monitors
With all the positive experiences, I am starting to feel some FOMO.
At nano we have not found them to be particularly useful and a maintenance headache (we have 2 per bay, ~30 total, one is always broken). Moving them during tool installs is a chore (vac tubing/new cables runs/fussy connectors) and the vac pumps consume non-trivial energy.
We use the MET One 6015 (0.5 micron). In our Class 100/ISO5 laminar flow areas, they very rarely read above zero unless we lose space pressurization, which is already caught by our DP sensors anyway. Because the capture window against the wall and below the HEPA is quite small, they just don't pick up much, though we do occasionally get readings in the Class 10k/ISO7 spaces.
Our original Basis of Design called for particle-counter-driven ACH, but we quickly replaced that with occupancy sensors. They are highly reliable at detecting the actual source of particles (people), act proactively, and have a much wider field of view.
Nick Menounos, PE
MIT.nano - Associate Director of Infrastructure
Cell: (508) 932-0938<tel:+15089320938>
From: labnetwork <labnetwork-bounces at mtl.mit.edu> On Behalf Of Carroll, David
Sent: Tuesday, March 24, 2026 12:13 PM
To: Nathan Aultman <naultman at creol.ucf.edu>
Cc: Network Fab <labnetwork at mtl.mit.edu>
Subject: Re: [labnetwork] Cleanroom Particle Monitors
Hi Dr. Dixon,
We too use the MetOne GT system and it has been a excellent device for us.
Dave
Wake Forest University
On Tue, Mar 24, 2026 at 12:09 PM Nathan Aultman <naultman at creol.ucf.edu<mailto:naultman at creol.ucf.edu>> wrote:
Dr. Dixon,
We use a MetOne GT-321. It is one of their older models. https://metone.com/product-categories/controlled-environments-clean-rooms/<https://urldefense.com/v3/__https:/metone.com/product-categories/controlled-environments-clean-rooms/__;!!O7_YSHcmd9jp3hj_4dEAcyQ!wquIoT7fitQJgL8WUUvYpQTUhW1WS3eJSY737geH720YLE57qXyReEyjj8ccctWXj9HiQqW49mLmDTB_tXleS9VIRg$>
Nathan C. Aultman
University of Central Florida
407-823-6852
naultman at creol.ucf.edu<mailto:naultman at creol.ucf.edu>
From: labnetwork <labnetwork-bounces at mtl.mit.edu<mailto:labnetwork-bounces at mtl.mit.edu>> On Behalf Of Alex Dixon
Sent: Monday, March 23, 2026 4:22 PM
To: Network Fab <labnetwork at mtl.mit.edu<mailto:labnetwork at mtl.mit.edu>>
Subject: [labnetwork] Cleanroom Particle Monitors
Hi Everyone, I was wondering what people use for particle measurement systems in their cleanrooms? We are trying to add active particle monitoring to our cleanroom facilities. I was looking at the lasair pro from "Particle Measuring Systems" https://www.pmeasuring.com/<https://urldefense.com/v3/__https:/www.pmeasuring.com/__;!!O7_YSHcmd9jp3hj_4dEAcyQ!wquIoT7fitQJgL8WUUvYpQTUhW1WS3eJSY737geH720YLE57qXyReEyjj8ccctWXj9HiQqW49mLmDTB_tXlL5nBvpg$> but university procurement is asking me to put together some other options.
-Alex
__________________________________________________________
Alex Dixon, Ph.D. (He/Him)
Lab Manager
Nanofabrication and Thin Film Deposition
Shared Instrument Facility
Colorado School of Mines
_______________________________________________
labnetwork mailing list
labnetwork at mtl.mit.edu<mailto:labnetwork at mtl.mit.edu>
https://mtl.mit.edu/mailman/listinfo.cgi/labnetwork<https://urldefense.com/v3/__https:/mtl.mit.edu/mailman/listinfo.cgi/labnetwork__;!!O7_YSHcmd9jp3hj_4dEAcyQ!wquIoT7fitQJgL8WUUvYpQTUhW1WS3eJSY737geH720YLE57qXyReEyjj8ccctWXj9HiQqW49mLmDTB_tXnENnKcgw$>
--
[https://ci3.googleusercontent.com/mail-sig/AIorK4waCuLiotTjsm78s5FfIEsmwYz7oR0pEuZ9zn1MLBu95Uy3kjsyJ9O0HL1LbKPw0V7KdqpEpSOgNr7Q]
David L. Carroll PhD.
Nano and Quantum Technologies Laboratory
Wake Forest University
95 W 32nd Street | Winston-Salem NC 27105 U.S.A.
Web. www.d<https://urldefense.com/v3/__http:/www.wfu.edu/*carroldl__;fg!!O7_YSHcmd9jp3hj_4dEAcyQ!wquIoT7fitQJgL8WUUvYpQTUhW1WS3eJSY737geH720YLE57qXyReEyjj8ccctWXj9HiQqW49mLmDTB_tXkY2sNDTQ$>avid-carroll.org<https://urldefense.com/v3/__http:/www.david-carroll.org/__;!!O7_YSHcmd9jp3hj_4dEAcyQ!wquIoT7fitQJgL8WUUvYpQTUhW1WS3eJSY737geH720YLE57qXyReEyjj8ccctWXj9HiQqW49mLmDTB_tXlkwJd_RA$>
Web. www.wake-nanotech.org<https://urldefense.com/v3/__http:/www.wake-nanotech.org/__;!!O7_YSHcmd9jp3hj_4dEAcyQ!wquIoT7fitQJgL8WUUvYpQTUhW1WS3eJSY737geH720YLE57qXyReEyjj8ccctWXj9HiQqW49mLmDTB_tXkz-s5PvA$>
[https://ci3.googleusercontent.com/mail-sig/AIorK4z4mqjdq5pfNYoHKKCsumtpAKnourN52vONGmx3KRmT3sbiPtaskOPIVOUev622dsuxBLeuZJ5Uvn0I]
The content of this email and any files transmitted with it may be confidential and intended solely for the use of the individual named. If you have received this email in error please let us know and delete the content from your system. You may NOT copy or disclose the information to anyone. We do not accept any liability if this email is used for an alternative purpose from which it is intended, nor to any third party in respect thereof. The sender does not accept liability for any errors or omissions in the contents of this message, which arise as a result of e-mail transmission. Unless we have agreed otherwise in writing, Sony DADC's Standard Terms and Conditions (https://www.sonydadc.com/wp-content/uploads/2024/03/Sony-DADC-Europe-Standard-TCs.pdf) of Business will apply to any services and-or disc/home-entertainment related products we provide to you, and our General Conditions of Purchase (https://www.sonydadc.com/wp-content/uploads/2024/03/SonyDADC_Purchasing_TCs.pdf) will apply to any goods and/or services we purchase from you.
-------------- next part --------------
An HTML attachment was scrubbed...
URL: <https://mtl.mit.edu/pipermail/labnetwork/attachments/20260512/1767f827/attachment.html>
-------------- next part --------------
A non-text attachment was scrubbed...
Name: image001.png
Type: image/png
Size: 242043 bytes
Desc: image001.png
URL: <https://mtl.mit.edu/pipermail/labnetwork/attachments/20260512/1767f827/attachment.png>
More information about the labnetwork
mailing list