    I have historically used both Angstrom Sciences and Lesker for
    various target materials. I had good luck with several exotic/custom
    targets from Angstrom, but in head-to-head for same material I have
    not seen any measurable distinction in film quality, longevity or
    contamination.<br>
    <pre class="moz-signature" cols="80">David A. Bunzow
User Facilities Program Manager
The Molecular Foundry
Materials Science Division
Lawrence Berkeley National Laboratory
1 Cyclotron Road        MS 67-3207
Berkeley, CA   94720

Office:  510-486-4574
FAX:  510-486-7424
Cell:  701-541-2354
</pre>
    <br>
    On 8/12/2011 4:01 AM, Morrison, Richard H., Jr. wrote:
    <blockquote
      cite="mid:94CDEF5D18F0BB4A85B1D78EFBDD6FDA0485DF17@exchbk1.draper.com"
      type="cite">
      <pre wrap="">Here at Draper Labs we use Materion (was Williams) 845-279-0900.

Sometimes we use Angstrom Sciences   <a class="moz-txt-link-abbreviated" href="http://www.angstromsciences.com">www.angstromsciences.com</a>

Rick


-----Original Message-----
From: <a class="moz-txt-link-abbreviated" href="mailto:labnetwork-bounces@mtl.mit.edu">labnetwork-bounces@mtl.mit.edu</a>
[<a class="moz-txt-link-freetext" href="mailto:labnetwork-bounces@mtl.mit.edu">mailto:labnetwork-bounces@mtl.mit.edu</a>] On Behalf Of Bill Flounders
Sent: Thursday, August 11, 2011 8:46 PM
To: Kevin McPeak
Cc: <a class="moz-txt-link-abbreviated" href="mailto:labnetwork@mtl.mit.edu">labnetwork@mtl.mit.edu</a>
Subject: Re: [labnetwork] Preferred sputtering target supplier (for
TCOs)

Lesker provides high quality targets.
The material you are 'targeting' is finicky.
If you have no evidence of contamination
and no issues with debonding, I would question
process parameters before Lesker's target quality.

Bill Flounders
UC Berkeley

Kevin McPeak wrote:
</pre>
      <blockquote type="cite">
        <pre wrap="">Dear labnetwork subscribers,

Do any of you have recommendations for suppliers for sputtering
targets? I have been using Lesker targets for my PVD75 sputterer. I am
perfectly happy with their metal targets but haven't had the best of
luck RF sputtering Al:ZnO films with their 2% Al2O3 /  98% ZnO target
(copper backed and Indium bonded). My issues may not be related to
their target at all but I am interested to hear if others on the list
feel strongly about certain target suppliers, especially for TCO
materials like Al:ZnO and ITO. Thanks in advance for your input.

Regards,
Kevin McPeak

</pre>
      </blockquote>
      <pre wrap="">
_______________________________________________
labnetwork mailing list
<a class="moz-txt-link-abbreviated" href="mailto:labnetwork@mtl.mit.edu">labnetwork@mtl.mit.edu</a>
<a class="moz-txt-link-freetext" href="https://www-mtl.mit.edu/mailman/listinfo.cgi/labnetwork">https://www-mtl.mit.edu/mailman/listinfo.cgi/labnetwork</a>

_______________________________________________
labnetwork mailing list
<a class="moz-txt-link-abbreviated" href="mailto:labnetwork@mtl.mit.edu">labnetwork@mtl.mit.edu</a>
<a class="moz-txt-link-freetext" href="https://www-mtl.mit.edu/mailman/listinfo.cgi/labnetwork">https://www-mtl.mit.edu/mailman/listinfo.cgi/labnetwork</a>
</pre>
    </blockquote>
  </body>
</html>