We are very happy with our (4)<a
href="http://www.laurell.com/index.php"> Laurell </a>spinners.
They are simple, well built, and relatively inexpensive. I bought a
new one for $4100 USD. In my opinion, simple spinners and hot plates
are more appropriate for university labs. Track coaters are very
complex and hard to maintain. <br>
<br>
<div class="moz-signature">-----------------<br>
Michael Rooks<br>
Yale Institute for Nanoscience & Quantum Engineering<br>
<a href="http://nano.yale.edu">nano.yale.edu</a><br>
<br>
<br>
<br>
</div>
<br>
On 08/23/2012 08:03 AM, Leif Johansen wrote:
<blockquote
cite="mid:39838FA4BF2F9A43AE3918CAD0F6AF171866F30881@WINEXCHANGE3.win.dtu.dk"
type="cite">
<meta http-equiv="Content-Type" content="text/html;
charset=ISO-8859-1">
<meta name="Generator" content="Microsoft Word 12 (filtered
medium)">
<!--[if !mso]><style>v\:* {behavior:url(#default#VML);}
o\:* {behavior:url(#default#VML);}
w\:* {behavior:url(#default#VML);}
.shape {behavior:url(#default#VML);}
</style><![endif]-->
<style><!--
/* Font Definitions */
@font-face
{font-family:Wingdings;
panose-1:5 0 0 0 0 0 0 0 0 0;}
@font-face
{font-family:Wingdings;
panose-1:5 0 0 0 0 0 0 0 0 0;}
@font-face
{font-family:Calibri;
panose-1:2 15 5 2 2 2 4 3 2 4;}
@font-face
{font-family:Tahoma;
panose-1:2 11 6 4 3 5 4 4 2 4;}
/* Style Definitions */
p.MsoNormal, li.MsoNormal, div.MsoNormal
{margin:0cm;
margin-bottom:.0001pt;
font-size:11.0pt;
font-family:"Calibri","sans-serif";}
a:link, span.MsoHyperlink
{mso-style-priority:99;
color:blue;
text-decoration:underline;}
a:visited, span.MsoHyperlinkFollowed
{mso-style-priority:99;
color:purple;
text-decoration:underline;}
p.MsoAcetate, li.MsoAcetate, div.MsoAcetate
{mso-style-priority:99;
mso-style-link:"Balloon Text Char";
margin:0cm;
margin-bottom:.0001pt;
font-size:8.0pt;
font-family:"Tahoma","sans-serif";}
p.MsoListParagraph, li.MsoListParagraph, div.MsoListParagraph
{mso-style-priority:34;
margin-top:0cm;
margin-right:0cm;
margin-bottom:0cm;
margin-left:36.0pt;
margin-bottom:.0001pt;
font-size:11.0pt;
font-family:"Calibri","sans-serif";}
span.EmailStyle17
{mso-style-type:personal-compose;
font-family:"Calibri","sans-serif";
color:windowtext;}
span.BalloonTextChar
{mso-style-name:"Balloon Text Char";
mso-style-priority:99;
mso-style-link:"Balloon Text";
font-family:"Tahoma","sans-serif";}
.MsoChpDefault
{mso-style-type:export-only;}
@page WordSection1
{size:612.0pt 792.0pt;
margin:3.0cm 2.0cm 3.0cm 2.0cm;}
div.WordSection1
{page:WordSection1;}
/* List Definitions */
@list l0
{mso-list-id:1089421349;
mso-list-type:hybrid;
mso-list-template-ids:967336754 67502081 67502083 67502085 67502081 67502083 67502085 67502081 67502083 67502085;}
@list l0:level1
{mso-level-number-format:bullet;
mso-level-text:\F0B7;
mso-level-tab-stop:none;
mso-level-number-position:left;
text-indent:-18.0pt;
font-family:Symbol;}
ol
{margin-bottom:0cm;}
ul
{margin-bottom:0cm;}
--></style><!--[if gte mso 9]><xml>
<o:shapedefaults v:ext="edit" spidmax="2050" />
</xml><![endif]--><!--[if gte mso 9]><xml>
<o:shapelayout v:ext="edit">
<o:idmap v:ext="edit" data="1" />
</o:shapelayout></xml><![endif]-->
<div class="WordSection1">
<p class="MsoNormal">Dear all, <o:p></o:p></p>
<p class="MsoNormal"><o:p> </o:p></p>
<p class="MsoNormal"><span lang="EN-US">In our lab we have a 20
years old Semiconductor Systems Inc. (SSI) track coater
which is on its last leg. I have noticed that quite a number
of you are using Silicon Valley Group (SVG) coaters. We are
presently considering if we should buy a refurbished SVG
coater as a replacement tool. I therefore have a few
questions:<o:p></o:p></span></p>
<p class="MsoNormal"><span lang="EN-US"><o:p> </o:p></span></p>
<p class="MsoListParagraph"
style="text-indent:-18.0pt;mso-list:l0 level1 lfo1"><!--[if !supportLists]--><span
style="font-family:Symbol" lang="EN-US"><span
style="mso-list:Ignore">·<span style="font:7.0pt
"Times New Roman""> </span></span></span><!--[endif]--><span
lang="EN-US">What is our experience with their up-time?<o:p></o:p></span></p>
<p class="MsoListParagraph"
style="text-indent:-18.0pt;mso-list:l0 level1 lfo1"><!--[if !supportLists]--><span
style="font-family:Symbol" lang="EN-US"><span
style="mso-list:Ignore">·<span style="font:7.0pt
"Times New Roman""> </span></span></span><!--[endif]--><span
lang="EN-US">How easy are they to service?<o:p></o:p></span></p>
<p class="MsoListParagraph"
style="text-indent:-18.0pt;mso-list:l0 level1 lfo1"><!--[if !supportLists]--><span
style="font-family:Symbol" lang="EN-US"><span
style="mso-list:Ignore">·<span style="font:7.0pt
"Times New Roman""> </span></span></span><!--[endif]--><span
lang="EN-US">Is the cost of ownership large, medium or
small?<o:p></o:p></span></p>
<p class="MsoListParagraph"
style="text-indent:-18.0pt;mso-list:l0 level1 lfo1"><!--[if !supportLists]--><span
style="font-family:Symbol" lang="EN-US"><span
style="mso-list:Ignore">·<span style="font:7.0pt
"Times New Roman""> </span></span></span><!--[endif]--><span
lang="EN-US">Is it still possible to find companies which
can provide spare parts and/or offer engineering services?<o:p></o:p></span></p>
<p class="MsoNormal"><span lang="EN-US"><o:p> </o:p></span></p>
<p class="MsoNormal"><span lang="EN-US">Best regards, <o:p></o:p></span></p>
<p class="MsoNormal"><span lang="EN-US"><o:p> </o:p></span></p>
<p class="MsoNormal"><span lang="EN-US">Leif<o:p></o:p></span></p>
<p class="MsoNormal"><span lang="EN-US"><o:p> </o:p></span></p>
<table class="MsoNormalTable"
style="width:300.0pt;border-collapse:collapse" border="0"
cellpadding="0" cellspacing="0" width="400">
<tbody>
<tr>
<td colspan="2" style="width:300.0pt;padding:0cm 0cm 0cm
0cm" valign="top" width="400">
<p class="MsoNormal"><b><span
style="font-size:8.0pt;font-family:"Arial","sans-serif";color:black">Leif
S. Johansen </span></b><b><span
style="font-size:8.0pt;font-family:"Arial","sans-serif";color:black"><o:p></o:p></span></b></p>
</td>
</tr>
<tr>
<td colspan="2" style="width:300.0pt;padding:0cm 0cm 0cm
0cm" valign="top" width="400">
<p class="MsoNormal"><span
style="font-size:8.0pt;font-family:"Arial","sans-serif";color:#9B9B9B">Head
of Operations</span><span
style="font-size:8.0pt;font-family:"Arial","sans-serif";color:#9B9B9B"><o:p></o:p></span></p>
</td>
</tr>
<tr>
<td colspan="2" style="width:300.0pt;padding:0cm 0cm 0cm
0cm" valign="top" width="400">
<p class="MsoNormal"><span
style="font-size:8.0pt;font-family:"Arial","sans-serif";color:black">DTU
Danchip </span><span
style="font-size:8.0pt;font-family:"Arial","sans-serif";color:black"><o:p></o:p></span></p>
</td>
</tr>
<tr>
<td colspan="2"
style="width:300.0pt;border:none;border-bottom:solid
#AEAEAE 1.0pt;padding:0cm 0cm 0cm 0cm" valign="top"
width="400">
<p class="MsoNormal" style="mso-line-height-alt:0pt"><span
style="font-size:8.0pt;font-family:"Arial","sans-serif";color:black">
</span><span
style="font-size:8.0pt;font-family:"Arial","sans-serif";color:black"><o:p></o:p></span></p>
</td>
</tr>
<tr>
<td style="width:262.5pt;padding:6.0pt 0cm 0cm 0cm"
valign="top" width="350">
<p class="MsoNormal"><b><span
style="font-size:8.0pt;font-family:"Arial","sans-serif";color:black">Technical
University of Denmark</span></b><b><span
style="font-size:8.0pt;font-family:"Arial","sans-serif";color:black"><o:p></o:p></span></b></p>
</td>
<td rowspan="7" style="width:37.5pt;padding:6.0pt 0cm 0cm
0cm" valign="top" width="50">
<p class="MsoNormal" style="text-align:right"
align="right"><span
style="font-size:8.0pt;font-family:"Arial","sans-serif";color:black"><img
id="Picture_x0020_1"
src="cid:part3.08080202.04040501@yale.edu"
alt="http://www.dtu.dk/images/DTU_email_logo_01.gif"
height="53" width="36"></span><span
style="font-size:8.0pt;font-family:"Arial","sans-serif";color:black"><o:p></o:p></span></p>
</td>
</tr>
<tr>
<td style="padding:0cm 0cm 0cm 0cm">
<p class="MsoNormal"><span
style="font-size:8.0pt;font-family:"Arial","sans-serif";color:black">Danchip
</span><span
style="font-size:8.0pt;font-family:"Arial","sans-serif";color:black"><o:p></o:p></span></p>
</td>
</tr>
<tr>
<td style="padding:0cm 0cm 0cm 0cm">
<p class="MsoNormal"><span
style="font-size:8.0pt;font-family:"Arial","sans-serif";color:black">Ørsteds
Plads, Byg. 347 </span><span
style="font-size:8.0pt;font-family:"Arial","sans-serif";color:black"><o:p></o:p></span></p>
</td>
</tr>
<tr>
<td style="padding:0cm 0cm 0cm 0cm">
<p class="MsoNormal"><span
style="font-size:8.0pt;font-family:"Arial","sans-serif";color:black">2800
Lyngby </span><span
style="font-size:8.0pt;font-family:"Arial","sans-serif";color:black"><o:p></o:p></span></p>
</td>
</tr>
<tr>
<td style="padding:0cm 0cm 0cm 0cm">
<p class="MsoNormal"><span
style="font-size:8.0pt;font-family:"Arial","sans-serif";color:black">Direct
+45 45255713 </span><span
style="font-size:8.0pt;font-family:"Arial","sans-serif";color:black"><o:p></o:p></span></p>
<p class="MsoNormal"><span
style="font-size:8.0pt;font-family:"Arial","sans-serif";color:black">Mobile
+45 25348992</span><span
style="font-size:8.0pt;font-family:"Arial","sans-serif";color:black"><o:p></o:p></span></p>
</td>
</tr>
<tr>
<td style="padding:0cm 0cm 0cm 0cm">
<p class="MsoNormal"><span
style="font-size:8.0pt;font-family:"Arial","sans-serif";color:black"><a
moz-do-not-send="true"
href="mailto:lesjo@danchip.dtu.dk"><span
style="color:blue">lesjo@danchip.dtu.dk</span></a>
</span><span
style="font-size:8.0pt;font-family:"Arial","sans-serif";color:black"><o:p></o:p></span></p>
</td>
</tr>
<tr>
<td style="padding:0cm 0cm 0cm 0cm">
<p class="MsoNormal"><span
style="font-size:8.0pt;font-family:"Arial","sans-serif";color:black"><a
moz-do-not-send="true"
href="http://www.danchip.dtu.dk/"><span
style="color:blue">www.danchip.dtu.dk/</span></a>
</span><span
style="font-size:8.0pt;font-family:"Arial","sans-serif";color:black"><o:p></o:p></span></p>
</td>
</tr>
</tbody>
</table>
<p class="MsoNormal"><o:p> </o:p></p>
<p class="MsoNormal"><o:p> </o:p></p>
</div>
<br>
<fieldset class="mimeAttachmentHeader"></fieldset>
<br>
<pre wrap="">_______________________________________________
labnetwork mailing list
<a class="moz-txt-link-abbreviated" href="mailto:labnetwork@mtl.mit.edu">labnetwork@mtl.mit.edu</a>
<a class="moz-txt-link-freetext" href="https://www-mtl.mit.edu/mailman/listinfo.cgi/labnetwork">https://www-mtl.mit.edu/mailman/listinfo.cgi/labnetwork</a>
</pre>
</blockquote>
</body>
</html>