<div>A local company is proposing to bend coaxial SS tubing to install a double containment gas line thus removing the need for welded 90° elbows. did you ever see that ? Any comment would be helpful ! </div>
<div><br>
</div>
<div>Thanks</div>
<div><br>
</div>
<div>Matthieu Nannini<br>
<div><br>
<div>Début du message réexpédié :</div>
<br class="x_Apple-interchange-newline">
<blockquote type="cite">
<div style="margin-top:0px; margin-right:0px; margin-bottom:0px; margin-left:0px">
<span style="font-family:'Helvetica'"><b>De: </b></span><span style="font-family:'Helvetica'">"Matthieu Nannini, Dr." <<a href="mailto:matthieu.nannini@mcgill.ca">matthieu.nannini@mcgill.ca</a>><br>
</span></div>
<div style="margin-top:0px; margin-right:0px; margin-bottom:0px; margin-left:0px">
<span style="font-family:'Helvetica'"><b>Objet: </b></span><span style="font-family:'Helvetica'"><b>Bending coaxial</b><br>
</span></div>
<div style="margin-top:0px; margin-right:0px; margin-bottom:0px; margin-left:0px">
<span style="font-family:'Helvetica'"><b>Date: </b></span><span style="font-family:'Helvetica'">15 décembre 2014 15:31:10 UTC−5<br>
</span></div>
<div style="margin-top:0px; margin-right:0px; margin-bottom:0px; margin-left:0px">
<span style="font-family:'Helvetica'"><b>À: </b></span><span style="font-family:'Helvetica'">Tom Britton <<a href="mailto:tbritton@criticalsystemsinc.com">tbritton@criticalsystemsinc.com</a>><br>
</span></div>
<br>
<div>Hi tom,<br>
<br>
A local company here can bend coaxial tubing. They quoted me 4800$ for the 2 lines BCl3 and SiCl4.<br>
<br>
What do you think of bending ? They told me the 1/4 wasn’t kinked at all.<br>
<br>
Matthieu<br>
<br>
</div>
</blockquote>
</div>
</div>
</div>
<div style="word-wrap:break-word">
<div>
<div class="x_AppleOriginalContents">
<blockquote type="cite">
<div></div>
</blockquote>
</div>
</div>
</div>
<div style="word-wrap:break-word">
<div>
<div>
<blockquote type="cite">
<div></div>
</blockquote>
</div>
<br>
</div>
</div>
</body>
</html>