    I am looking for information on how to fix an issue I have with our
    Perkin Elmer sputter tool. The system was working reasonably, but
    now when we run the system there is alot of arcing. It is not
    related to the target material or if we use a different target
    position. At 100 W there is no arcing and once we go above that,
    normally we use 700 W with this system for deposition of HfOx, we
    observe the arcing issue. This is not a continuous arc, but very
    sporadic events and has been leaving visible damage to the dark
    shields and the chamber walls. I have cleaned the dark shields,
    chamber wall, and sample stage with sandpaper and wipe all the
    surfaces with solvents, but that did not seem to have an affect on
    the arcing issue. <br>
    <br>
    This tool has also had a long issue with RF leakage effecting the
    mass flow controllers and RF tuning unit. Past lab users have tried
    to ground all the instruments that were effected but with minimal
    improvement.<br>
    <br>
    Any information or help would be greatly appreciated.<br>
    <br>
    Chito Kendrick<br>
    <br>
    <div class="moz-signature">-- <br>
      <a href="https://sites.google.com/site/chitokendrickphd/">Chito
        Kendrick Ph.D.</a><br>
      <br>
      Director of the Microfabrication Facility<br>
      Research Assistant Professor<br>
      Electrical and Computer Engineering<br>
      Michigan Technological University<br>
      Room 436 M&M Building<br>
      1400 Townsend Dr.<br>
      Houghton, Michigan 49931-1295<br>
      <br>
      814-308-4255<br>
    </div>
  </body>
</html>