<div dir="ltr"><div><div><div><div><div><div><div><div><div>Hi,<br><br></div>We use a 'Coherent COMPex Pro 102F' excimer laser (248 nm, KrF) as the laser source for pulsed laser deposition. Recently, close to 30 s into the deposition run at 5 Hz (150 pulses), the pulsing stopped and 'rec. error' was printed on the display of the laser controller. Has anyone ever encountered such an error? If yes, what does it mean and what do I need to do to correct it? There was a power surge in the lab a day before this happened but at that time, although the laser was connected to the power lines, it was turned off. Could this be an effect of the surge?<br><br></div>Some background:<br><br></div>-We operate the laser using the controller. No external triggering<br></div>- Recent gas mixture refill was <20 days before pulsing<br></div>- Laser is used routinely - no long periods of dormancy<br></div><br><br></div>Thank you!<br></div><br></div>Regards,<br clear="all"><div><div><div><div><div><div><div><div><div><div><div><br>-- <br><div class="gmail_signature"><div dir="ltr"><div><div dir="ltr"><div><div dir="ltr"><div><div><div>Pramod Ravindra<br></div>PhD Candidate<br></div>Centre for Nano-Science and Engineering (CeNSE)<br></div>Indian Institute of Science, Bangalore<br><div><div><div><div>+91-9916890128</div></div></div></div></div></div></div></div></div></div>
</div></div></div></div></div></div></div></div></div></div></div></div>