<div dir="ltr"><div><div><div>Hi Everyone,<br><br></div>I'm a relatively new lab engineer at the Idaho Micro-fabrication Lab at Boise State.  I've been looking at the archives and recognize a few names. <br><br>I am in need of schematics for a thermco minibrute MB-80 furnace. Specifically the heater controllers as I need to calibrate the temp but when I opened the controller up there are about 20 different pots. If anyone has a copy of the schematics or a calibration procedure that they could send a copy to me I would greatly appreciate it. <br><br></div>Thanks<br></div>Travis <br></div>