<p>Hi Esta, we buy all of our plates from Nanofilm
(<a class="moz-txt-link-freetext" href="http://www.nanofilm.com/">http://www.nanofilm.com/</a>) in California with chrome and AZ1518
resist. We don't have any special storage conditions in the clean
room other than yellow light. They do seem to expire in a year or
two. Also, unless you are working with DUV, I wouldn't spend the
extra for the quartz plates. We also use Heidelberg systems and
they work quite well for us. Let me know if you have any other
questions.</p>
<p>Thanks,<br>
Nathanael<br>
</p>
<br>
<div class="moz-cite-prefix">On 2017-08-18 6:17 AM, Abelev, Esta
wrote:<br>
</div>
<blockquote type="cite"
cite="mid:SN2PR04MB22054AF319BFFD6F4E342130C5800@SN2PR04MB2205.namprd04.prod.outlook.com">
<meta http-equiv="Content-Type" content="text/html;
charset=windows-1252">
<meta name="Generator" content="Microsoft Word 15 (filtered
medium)">
<style><!--
/* Font Definitions */
@font-face
{font-family:"Cambria Math";
panose-1:2 4 5 3 5 4 6 3 2 4;}
@font-face
{font-family:Calibri;
panose-1:2 15 5 2 2 2 4 3 2 4;}
@font-face
{font-family:Atlanta;}
/* Style Definitions */
p.MsoNormal, li.MsoNormal, div.MsoNormal
{margin:0cm;
margin-bottom:.0001pt;
font-size:11.0pt;
font-family:"Calibri",sans-serif;}
a:link, span.MsoHyperlink
{mso-style-priority:99;
color:#0563C1;
text-decoration:underline;}
a:visited, span.MsoHyperlinkFollowed
{mso-style-priority:99;
color:#954F72;
text-decoration:underline;}
span.EmailStyle17
{mso-style-type:personal-compose;
font-family:"Calibri",sans-serif;
color:windowtext;}
.MsoChpDefault
{mso-style-type:export-only;
font-family:"Calibri",sans-serif;}
@page WordSection1
{size:612.0pt 792.0pt;
margin:72.0pt 72.0pt 72.0pt 72.0pt;}
div.WordSection1
{page:WordSection1;}
--></style><!--[if gte mso 9]><xml>
<o:shapedefaults v:ext="edit" spidmax="1026" />
</xml><![endif]--><!--[if gte mso 9]><xml>
<o:shapelayout v:ext="edit">
<o:idmap v:ext="edit" data="1" />
</o:shapelayout></xml><![endif]-->
<div class="WordSection1">
<p class="MsoNormal">Dear Colleagues,<o:p></o:p></p>
<p class="MsoNormal"><o:p> </o:p></p>
<p class="MsoNormal">Our facility getting it first Heidelberg
laser write tool. I would like to get advice where to buy
quartz or Soda lime plates with Cr (maybe even with resist) to
make masks.<o:p></o:p></p>
<p class="MsoNormal">In addition, if some can comment how to
store them in the cleanroom.<o:p></o:p></p>
<p class="MsoNormal"><o:p> </o:p></p>
<p class="MsoNormal">Thank you, Esta<o:p></o:p></p>
<p class="MsoNormal"><o:p> </o:p></p>
<p class="MsoNormal"><o:p> </o:p></p>
<p class="MsoNormal"><span
style="font-size:9.0pt;font-family:Atlanta">-----------------------</span><o:p></o:p></p>
<p class="MsoNormal"><b><span
style="font-size:9.0pt;font-family:Atlanta">Esta Abelev,
PhD</span></b><o:p></o:p></p>
<p class="MsoNormal"><span
style="font-size:9.0pt;font-family:Atlanta">Technical
Director,<i> </i>Petersen Institute of NanoScience and
Engineering </span><o:p></o:p></p>
<p class="MsoNormal"><span
style="font-size:9.0pt;font-family:Atlanta">University of
Pittsburgh | 3700 O’Hara Street | 636| Pittsburgh, PA 15261</span><o:p></o:p></p>
<p class="MsoNormal"><span
style="font-size:9.0pt;font-family:Atlanta">412-383-4096 | <a
href="mailto:eabelev@pitt.edu" moz-do-not-send="true"><span
style="color:#0066CC;text-decoration:none">eabelev@pitt.edu</span></a> | <a
href="https://na01.safelinks.protection.outlook.com/?url=http%3A%2F%2Fwww.nano.pitt.edu%2F&data=01%7C01%7Ceabelev%40pitt.edu%7C9f5bd58ba84940765cf308d4024fbe18%7C9ef9f489e0a04eeb87cc3a526112fd0d%7C1&sdata=3KfbG5VbshqdoIAPxvX%2F2s1UeU7ultmBoZmm%2FaZ2Itc%3D&reserved=0"
moz-do-not-send="true"><span
style="color:purple;text-decoration:none">nano.pitt.edu</span></a></span><o:p></o:p></p>
<p class="MsoNormal"><span style="color:black"><o:p> </o:p></span></p>
<p class="MsoNormal"><o:p> </o:p></p>
</div>
<br>
<fieldset class="mimeAttachmentHeader"></fieldset>
<br>
<pre wrap="">_______________________________________________
labnetwork mailing list
<a class="moz-txt-link-abbreviated" href="mailto:labnetwork@mtl.mit.edu">labnetwork@mtl.mit.edu</a>
<a class="moz-txt-link-freetext" href="https://www-mtl.mit.edu/mailman/listinfo.cgi/labnetwork">https://www-mtl.mit.edu/mailman/listinfo.cgi/labnetwork</a>
</pre>
</blockquote>
<br>
<div class="moz-signature">
<div><br>
</div>
<div>
<hr>
<span style="font-family: arial,helvetica,sans-serif;"
data-mce-style="font-family: arial,helvetica,sans-serif;"><strong>Nathanael
Sieb</strong></span><br>
<span style="font-family: arial,helvetica,sans-serif; font-size:
x-small;" data-mce-style="font-family:
arial,helvetica,sans-serif; font-size: x-small;"> Director of
Operations and Administration</span><br>
<p class="HeaderFooter" style="line-height: 110%; margin: 0px;
text-align: left;" data-mce-style="line-height: 110%; margin:
0px; text-align: left;" align="right">
<span style="font-family: arial,helvetica,sans-serif;
font-size: small;" data-mce-style="font-family:
arial,helvetica,sans-serif; font-size: small;">
<span style="line-height: 110%; color: #014b8a;"
data-mce-style="line-height: 110%; color: #014b8a;"
lang="EN-US">4D LABS, Simon Fraser University </span>
<span style="line-height: 110%; color: #014b8a;"
data-mce-style="line-height: 110%; color: #014b8a;"
lang="EN-US">8888 University Drive, Burnaby, B.C. V5A 1S6</span>
</span>
</p>
<p class="HeaderFooter" style="line-height: 110%; margin: 0px;
text-align: left;" data-mce-style="line-height: 110%; margin:
0px; text-align: left;" align="right">
<span style="font-family: arial,helvetica,sans-serif;
font-size: small;" data-mce-style="font-family:
arial,helvetica,sans-serif; font-size: small;">
<span style="color: #ff4200;" data-mce-style="color:
#ff4200;" lang="EN-US">E </span>
<span style="color: #014b8a;" data-mce-style="color:
#014b8a;" lang="EN-US"><a class="moz-txt-link-abbreviated" href="mailto:sieb@4dlabs.ca">sieb@4dlabs.ca</a> </span>
<span style="color: #ff4200;" data-mce-style="color:
#ff4200;" lang="EN-US">T </span>
<span style="color: #014b8a;" data-mce-style="color:
#014b8a;" lang="EN-US">778.782.8084 </span>
<span style="color: #ff4200;" data-mce-style="color:
#ff4200;" lang="EN-US">F </span>
<span style="color: #014b8a;" data-mce-style="color:
#014b8a;" lang="EN-US">778.782.3765 </span>
<span style="color: #ff4200;" data-mce-style="color:
#ff4200;" lang="EN-US">W </span>
<span style="color: #014b8a;" data-mce-style="color:
#014b8a;" lang="EN-US"><a href="http://www.4dlabs.ca"
data-mce-href="http://www.4dlabs.ca">www.4dlabs.ca</a></span>
</span>
</p>
<p class="HeaderFooter" style="line-height: 400%; margin: 0px;
text-align: left;" data-mce-style="line-height: 400%; margin:
0px; text-align: left;" align="right">
<span style="font-family: arial,helvetica,sans-serif;"
data-mce-style="font-family: arial,helvetica,sans-serif;">
<span style="font-size: small;" data-mce-style="font-size:
small;">
<span style="line-height: 400%; color: #014b8a;"
data-mce-style="line-height: 400%; color: #014b8a;"
lang="EN-US">
<a href="https://www.4dlabs.ca"
data-mce-href="https://www.4dlabs.ca"><img
data-mce-src="http://www.4dlabs.ca/content/dam/sfu/4dlabs/images/4D-logo-tiny.png"
src="http://www.4dlabs.ca/content/dam/sfu/4dlabs/images/4D-logo-tiny.png"
height="32" width="32"></a>
<a href="https://www.linkedin.com/company/sfu-4d-labs"
data-mce-href="https://www.linkedin.com/company/sfu-4d-labs"><img
data-mce-src="http://www.4dlabs.ca/content/dam/sfu/4dlabs/images/linkedin_circle_color.jpg"
src="http://www.4dlabs.ca/content/dam/sfu/4dlabs/images/linkedin_circle_color.jpg"
height="32" width="32"></a>
<a href="https://twitter.com/4D_LABS"
data-mce-href="https://twitter.com/4D_LABS"><img
data-mce-src="http://www.4dlabs.ca/content/dam/sfu/4dlabs/images/twitter_circle_color.jpg"
src="http://www.4dlabs.ca/content/dam/sfu/4dlabs/images/twitter_circle_color.jpg"
height="32" width="32"></a>
<a href="https://www.facebook.com/4dlabs"
data-mce-href="https://www.facebook.com/4dlabs"><img
data-mce-src="http://www.4dlabs.ca/content/dam/sfu/4dlabs/images/facebook_circle_color.jpg"
src="http://www.4dlabs.ca/content/dam/sfu/4dlabs/images/facebook_circle_color.jpg"
height="32" width="32"></a>
</span>
</span>
</span>
</p>
<br>
</div>
</div>
</body>
</html>