<div class="">We will be trying to sputter Ni/Cr (50/50 wt%) on Alumina wafers and the thickness range will be between 30-50 nm. We are using the tool, Intlvac Nanochrome 1.</div>
<div class="">Since the material is magnetic, I was wondering if anyone would send us some suggestions on the process parameters to be used. There are several published reports on this but I wanted to check with</div>
<div class="">anyone who has some experience with this specific material.</div>
<div class=""><br class="">
</div>
<div class="">Any comments/suggestions will be much appreciated.</div>
<div class=""><br class="">
</div>
<div class="">Thanks</div>
<div class="">Aju</div>
<div class=""><br class="">
<div class=""><br class="">
</div>
<div class=""><br class="">
<div class=""><i class=""><font color="#0096ff" class="">Aju Jugessur, Ph.D.<br class="">
Director, University of Iowa Microfabrication Facility (UIMF)<br class="">
Optical Science and Technology Center<br class="">
Professor Adjunct, Physics and Astronomy<br class="">
University of Iowa<br class="">
Office: IATL 202, Tel: 319-3532342<br class="">
Labs: IATL 170, 172, 174<br class="">
<a href="https://ostc.uiowa.edu/uimf" class="">https://ostc.uiowa.edu/uimf</a></font></i><br class="">
<br class="">
<br class="">
<br class="">
<br class="">
<br class="">
</div>
<br class="">
</div>
</div>
</body>
</html>