<div dir="auto">Dear Mike,<div dir="auto"><br></div><div dir="auto">That is a good point. We should totally do that and will. What else do you think this black stuff could be?</div><div dir="auto"><br></div><div dir="auto">Regards,</div><div dir="auto">Kevin<br><br><div data-smartmail="gmail_signature" dir="auto">--<br>Kevin McPeak<br>Assistant Professor<br>Department of Chemical Engineering<br>Louisiana State University<br>email: <a href="mailto:kmcpeak@lsu.edu">kmcpeak@lsu.edu</a><br>phone: 225-578-0058</div></div></div><div class="gmail_extra"><br><div class="gmail_quote">On Oct 28, 2017 09:58, "Mike Young" <<a href="mailto:myoung6@nd.edu">myoung6@nd.edu</a>> wrote:<br type="attribution"><blockquote class="gmail_quote" style="margin:0 0 0 .8ex;border-left:1px #ccc solid;padding-left:1ex">
  
    
  
  <div text="#000000" bgcolor="#FFFFFF">
    <p>Hi Kevin. Have you confirmed the deposits are in fact carbon?
      Scrape some off and perfom EDX in a SEM, for example?</p>
    <p>--Mike<br>
    </p>
    <br>
    <div class="m_-8801171658933078857moz-cite-prefix">On 10/28/2017 12:19 AM, Kevin McPeak
      wrote:<br>
    </div>
    <blockquote type="cite">
      <pre>Dear Colleagues,

In my lab at LSU we are interested in evaporating Au under high Ar
pressures, 10 - 50 mTorr. We are using Ar 5.0 purity (99.999%), which
has a THC of 1 ppm.

Our procedure is such:

1). Pump chamber down to low -7 Torr range
2). Inject 30 SCCM Ar and throttle gate valve to the desired pressure
(say 50 mTorr)
3). Increase power to Tungsten boat till Au pellets evaporate

When we vent the chamber <u><b>we notice a lot of carbon deposition</b></u> near the
outlet of the Ar line (see attached image). We have a THC of 1 ppm in
the Ar tank. We also tried hooking up a GP-100 gas purifier from RD
Mathis. Unfortunately, that didn't solve the problem, still lots of
carbon deposition in the chamber. The GP-100 is currently connected
upstream from the MFC. I am using SS tubes with all VCR fittings
(total length 6 ft). We could move the GP-100 closer to the chamber,
post-MFC.

Based on the photo I think it is pretty clear that the carbon is
coming from the Ar. So my current thought is that either I have a leak
in my tubes post GP-100 or I need to flame bake the lines (I have not
done this). I am trying to get access to an RGA to investigate this
more quantitatively. I do have access to a He checker so I could try
pumping on the Ar lines.

Have any of you seen Carbon contamination like this before when doing
high-pressure evap (I know that is not a normal thing)? I am curious
what people think. Thanks!

Regards,
Kevin

</pre>
    </blockquote>
    <br>
    <pre class="m_-8801171658933078857moz-signature" cols="72">-- 
Michael P. Young                                <a href="tel:(574)%20631-3268" value="+15746313268" target="_blank">(574) 631-3268</a> (office)
Nanofabrication Specialist                      <a href="tel:(574)%20631-4393" value="+15746314393" target="_blank">(574) 631-4393</a> (fax)
Department of Electrical Engineering            <a href="tel:(765)%20637-3784" value="+17656373784" target="_blank">(765) 637-3784</a> (cell)
University of Notre Dame                         <a class="m_-8801171658933078857moz-txt-link-abbreviated" href="mailto:mike.young@nd.edu" target="_blank">mike.young@nd.edu</a>
B-38 Stinson-Remick Hall
Notre Dame, IN 46556-5637</pre>
  </div>

</blockquote></div></div>