<html xmlns:v="urn:schemas-microsoft-com:vml" xmlns:o="urn:schemas-microsoft-com:office:office" xmlns:w="urn:schemas-microsoft-com:office:word" xmlns:m="http://schemas.microsoft.com/office/2004/12/omml" xmlns="http://www.w3.org/TR/REC-html40">
<head>
<meta http-equiv="Content-Type" content="text/html; charset=us-ascii">
<meta name="Generator" content="Microsoft Word 15 (filtered medium)">
<style><!--
/* Font Definitions */
@font-face
        {font-family:"Cambria Math";
        panose-1:2 4 5 3 5 4 6 3 2 4;}
@font-face
        {font-family:Calibri;
        panose-1:2 15 5 2 2 2 4 3 2 4;}
@font-face
        {font-family:Atlanta;
        panose-1:0 0 0 0 0 0 0 0 0 0;}
/* Style Definitions */
p.MsoNormal, li.MsoNormal, div.MsoNormal
        {margin:0in;
        margin-bottom:.0001pt;
        font-size:11.0pt;
        font-family:"Calibri",sans-serif;}
a:link, span.MsoHyperlink
        {mso-style-priority:99;
        color:#0563C1;
        text-decoration:underline;}
a:visited, span.MsoHyperlinkFollowed
        {mso-style-priority:99;
        color:#954F72;
        text-decoration:underline;}
span.EmailStyle17
        {mso-style-type:personal;
        font-family:"Calibri",sans-serif;
        color:windowtext;}
span.EmailStyle18
        {mso-style-type:personal-reply;
        font-family:"Calibri",sans-serif;
        color:#1F497D;}
.MsoChpDefault
        {mso-style-type:export-only;
        font-size:10.0pt;}
@page WordSection1
        {size:8.5in 11.0in;
        margin:1.0in 1.0in 1.0in 1.0in;}
div.WordSection1
        {page:WordSection1;}
--></style><!--[if gte mso 9]><xml>
<o:shapedefaults v:ext="edit" spidmax="1026" />
</xml><![endif]--><!--[if gte mso 9]><xml>
<o:shapelayout v:ext="edit">
<o:idmap v:ext="edit" data="1" />
</o:shapelayout></xml><![endif]-->
</head>
<body lang="EN-US" link="#0563C1" vlink="#954F72">
<div class="WordSection1">
<p class="MsoNormal"><span style="color:#1F497D">Hello Esta,<o:p></o:p></span></p>
<p class="MsoNormal"><span style="color:#1F497D"><o:p> </o:p></span></p>
<p class="MsoNormal"><span style="color:#1F497D">Have you considered using a shadow mask and an evaporator? Substrate shape and topography could present a challenge, and some fixturing would be required, but no resist would be required and with a great enough
 throw distance (on the order of 60cm+), your temperatures should stay cool enough to get the job done.<o:p></o:p></span></p>
<p class="MsoNormal"><span style="color:#1F497D"><o:p> </o:p></span></p>
<p class="MsoNormal"><span style="color:#1F497D">Best,<o:p></o:p></span></p>
<p class="MsoNormal"><span style="color:#1F497D"><br>
Carsen<o:p></o:p></span></p>
<p class="MsoNormal"><span style="color:#1F497D"><o:p> </o:p></span></p>
<p class="MsoNormal"><span style="color:#1F497D"><o:p> </o:p></span></p>
<div>
<div style="border:none;border-top:solid #E1E1E1 1.0pt;padding:3.0pt 0in 0in 0in">
<p class="MsoNormal"><b>From:</b> labnetwork-bounces@mtl.mit.edu [mailto:labnetwork-bounces@mtl.mit.edu]
<b>On Behalf Of </b>Abelev, Esta<br>
<b>Sent:</b> Wednesday, January 24, 2018 11:57 AM<br>
<b>To:</b> labnetwork@mtl.mit.edu<br>
<b>Subject:</b> [labnetwork] Device on PDMS<o:p></o:p></p>
</div>
</div>
<p class="MsoNormal"><o:p> </o:p></p>
<p class="MsoNormal">Dear All,<o:p></o:p></p>
<p class="MsoNormal"><o:p> </o:p></p>
<p class="MsoNormal">We have a group here that is interesting to make some gold electrodes on PDMS substrates.
<o:p></o:p></p>
<p class="MsoNormal">We found it is very challenging to bake the resist on PDMS dew to it temp. sensitivity (shrinks).<o:p></o:p></p>
<p class="MsoNormal">Can anyone advise us on how to do it, any tricks? <o:p></o:p></p>
<p class="MsoNormal"><o:p> </o:p></p>
<p class="MsoNormal">Thank you, Esta<o:p></o:p></p>
<p class="MsoNormal"><o:p> </o:p></p>
<p class="MsoNormal"><span style="font-size:9.0pt;font-family:"Atlanta",serif">-----------------------</span><o:p></o:p></p>
<p class="MsoNormal"><b><span style="font-size:9.0pt;font-family:"Atlanta",serif">Esta Abelev, PhD</span></b><o:p></o:p></p>
<p class="MsoNormal"><span style="font-size:9.0pt;font-family:"Atlanta",serif">Technical Director,<i> </i>Petersen Institute of NanoScience and Engineering </span><o:p></o:p></p>
<p class="MsoNormal"><span style="font-size:9.0pt;font-family:"Atlanta",serif">University of Pittsburgh | 3700 O’Hara Street | 636| Pittsburgh, PA 15261</span><o:p></o:p></p>
<p class="MsoNormal"><span style="font-size:9.0pt;font-family:"Atlanta",serif">412-383-4096 | <a href="mailto:eabelev@pitt.edu"><span style="color:#0066CC;text-decoration:none">eabelev@pitt.edu</span></a> | <a href="https://na01.safelinks.protection.outlook.com/?url=http%3A%2F%2Fwww.nano.pitt.edu%2F&data=01%7C01%7Ceabelev%40pitt.edu%7C9f5bd58ba84940765cf308d4024fbe18%7C9ef9f489e0a04eeb87cc3a526112fd0d%7C1&sdata=3KfbG5VbshqdoIAPxvX%2F2s1UeU7ultmBoZmm%2FaZ2Itc%3D&reserved=0"><span style="color:purple;text-decoration:none">nano.pitt.edu</span></a></span><o:p></o:p></p>