<div dir="ltr">Hello Mathilde,<div><br></div><div>Here at LNF (U-Michigan), we have the same problem. We have, also, tried to buy just the curing agent, but no luck. If you manage to convince Dow to sell us extra curing agent, please let us know!.</div><div><br></div><div>Pilar</div><div><br></div><div><br></div><div><br></div></div><div class="gmail_extra"><br><div class="gmail_quote">On Fri, Mar 2, 2018 at 2:24 AM, Mathilde Isabelle Barriet <span dir="ltr"><<a href="mailto:mathilde.i.barriet@ntnu.no" target="_blank">mathilde.i.barriet@ntnu.no</a>></span> wrote:<br><blockquote class="gmail_quote" style="margin:0 0 0 .8ex;border-left:1px #ccc solid;padding-left:1ex">Dear All<br>
As many of you we are using Sylgard 184. In Norway we have no other choice than buying it as a kit (1kg elastomer + 100g of curing agent).<br>
For some unknown reasons we have many cans of elastomers unused and no curing agent to go with... I have been trying to buy the curing agent alone through different channels (our supplier, dow corning) but with no success.<br>
Any of you has any advice or contacts so I can get the curing agent only.<br>
Thanks<br>
Kind regards<br>
Mathilde<br>
<br>
Senior Engineer<br>
NTNU NanoLab<br>
----------------------------<br>
Sem Sælands vei 14, K1-113<br>
NO-7491 Trondheim<br>
+47 91 89 72 08<br>
<a href="http://www.ntnu.no/nanolab" rel="noreferrer" target="_blank">www.ntnu.no/nanolab</a><br>
<br>
<br>
<br>
______________________________<wbr>_________________<br>
labnetwork mailing list<br>
<a href="mailto:labnetwork@mtl.mit.edu">labnetwork@mtl.mit.edu</a><br>
<a href="https://mtl.mit.edu/mailman/listinfo.cgi/labnetwork" rel="noreferrer" target="_blank">https://mtl.mit.edu/mailman/<wbr>listinfo.cgi/labnetwork</a><br>
</blockquote></div><br><br clear="all"><div><br></div>-- <br><div class="gmail_signature" data-smartmail="gmail_signature"><div dir="ltr"><div><div dir="ltr"><div><div dir="ltr"><div><div dir="ltr"><div><div dir="ltr"><font style="background-color:rgb(255,255,255)"><font face="tahoma, sans-serif" color="#0000ff" size="2">Pilar Herrera-Fierro, Ph.D.<br>LNF User Services Director<br>Lurie Nanofabrication Facility<br>University of Michigan</font><br></font><br>RM 1239 EECS Building<br>1301 Beal Ave.<br>Ann Arbor, MI 48109-2122<br><br><b>Cell</b> 734 646 1399<br><br>(734) 646 1399<div><br></div><div><a href="http://www.lnf.umich.edu" target="_blank">www.lnf.umich.edu</a></div><div><br><br><br></div></div></div></div></div></div></div></div></div></div></div>
</div>