<html><head><meta http-equiv="content-type" content="text/html; charset=utf-8"></head><body dir="auto">I’ve never tried ordering only curing agent, but one of the distributors we use for kits also lists it as a stand-alone product (albeit in rather large quantities):<div><br></div><div><a href="https://www.ellsworth.com/cart/add-to-cart/?item=184-CURING-AGENT-20.4KG-PL&qty=1">https://www.ellsworth.com/cart/add-to-cart/?item=184-CURING-AGENT-20.4KG-PL&qty=1</a></div><div><br><div id="AppleMailSignature">Thanks,<div>John</div><div><span class="Apple-style-span" style="-webkit-tap-highlight-color: rgba(26, 26, 26, 0.294118);"><br></span></div><div><span class="Apple-style-span" style="-webkit-tap-highlight-color: rgba(26, 26, 26, 0.292969); -webkit-composition-fill-color: rgba(175, 192, 227, 0.230469); -webkit-composition-frame-color: rgba(77, 128, 180, 0.230469);">----</span></div><div><span class="Apple-style-span" style="-webkit-tap-highlight-color: rgba(26, 26, 26, 0.296875); -webkit-composition-fill-color: rgba(175, 192, 227, 0.230469); -webkit-composition-frame-color: rgba(77, 128, 180, 0.230469); ">Sent from my mobile device</span></div><div><span class="Apple-style-span" style="-webkit-tap-highlight-color: rgba(26, 26, 26, 0.296875); -webkit-composition-fill-color: rgba(175, 192, 227, 0.230469); -webkit-composition-frame-color: rgba(77, 128, 180, 0.230469); "><br></span></div><div>Ioannis (John) Kymissis</div><div>Associate Professor, Electrical Engineering</div><div>Columbia University SEAS</div><div>500 W120th Street</div><div>Room 1300/MC 4712</div><div>New York, NY 10027</div><div>Tel: 347-850-0235</div><div>Fax: 212-932-9421</div><div><a href="mailto:johnkym@ee.columbia.edu">johnkym@ee.columbia.edu</a></div><div><a href="http://kymissis.columbia.edu">http://kymissis.columbia.edu</a></div></div><div><br>On Mar 2, 2018, at 2:24 AM, Mathilde Isabelle Barriet <<a href="mailto:mathilde.i.barriet@ntnu.no">mathilde.i.barriet@ntnu.no</a>> wrote:<br><br></div><blockquote type="cite"><div><span>Dear All</span><br><span>As many of you we are using Sylgard 184. In Norway we have no other choice than buying it as a kit (1kg elastomer + 100g of curing agent).</span><br><span>For some unknown reasons we have many cans of elastomers unused and no curing agent to go with... I have been trying to buy the curing agent alone through different channels (our supplier, dow corning) but with no success.</span><br><span>Any of you has any advice or contacts so I can get the curing agent only.</span><br><span>Thanks</span><br><span>Kind regards</span><br><span>Mathilde</span><br><span></span><br><span>Senior Engineer</span><br><span>NTNU NanoLab</span><br><span>----------------------------</span><br><span>Sem Sælands vei 14, K1-113</span><br><span>NO-7491 Trondheim</span><br><span>+47 91 89 72 08</span><br><span><a href="http://www.ntnu.no/nanolab">www.ntnu.no/nanolab</a></span><br><span></span><br><span></span><br><span></span><br><span>_______________________________________________</span><br><span>labnetwork mailing list</span><br><span><a href="mailto:labnetwork@mtl.mit.edu">labnetwork@mtl.mit.edu</a></span><br><span><a href="https://mtl.mit.edu/mailman/listinfo.cgi/labnetwork">https://mtl.mit.edu/mailman/listinfo.cgi/labnetwork</a></span><br><span></span><br></div></blockquote></div></body></html>