<div dir="ltr">
<div class="gmail_default" style="font-family:monospace,monospace;font-size:small">
Dear colleagues</div>
<div class="gmail_default" style="font-family:monospace,monospace;font-size:small">
<br>
</div>
<div class="gmail_default" style="font-family:monospace,monospace;font-size:small">
We are going to buy an RIE/PECVD system. Some vendors offer one-piece aluminum chambers while others offer welded stainless steel.</div>
<div class="gmail_default" style="font-family:monospace,monospace;font-size:small">
<br>
</div>
<div class="gmail_default" style="font-family:monospace,monospace;font-size:small">
I understand that one-piece metal is good for keeping the vacuum, but which is more important (one-piece aluminum vs. welded stainless steel), if we have to choose one configuration?</div>
<div class="gmail_default" style="font-family:monospace,monospace;font-size:small">
<br>
</div>
<div class="gmail_default" style="font-family:monospace,monospace;font-size:small">
Any suggestions and insights are highly welcome.</div>
<div class="gmail_default" style="font-family:monospace,monospace;font-size:small">
<br>
</div>
<div class="gmail_default" style="font-family:monospace,monospace;font-size:small">
Shane</div>
<div dir="ltr" class="gmail_signature" data-smartmail="gmail_signature">
<div dir="ltr">
<div dir="ltr">
<div dir="ltr">
<div dir="ltr">
<div dir="ltr"></div>
</div>
</div>
</div>
</div>
</div>
</div>
</body>
</html>