<div>Hi all,</div>
<div>We have a user request for deposition of Barium from BaO powder using evaporation. The user is not too particular about the stoichiometry of the deposited film – both Ba or BaO or a mixture thereof are acceptable at this stage. I will try to make pellets
out of the powder before we evaporate. </div>
<div>I wanted to run it by the labnetwork community to see if there’re particular things to be careful about e.g.</div>
<ol style="margin:0;padding-left:36pt;">
<li>Should we use e-beam or thermal evaporation technique?</li><li>What kind of boat/crucible material should be used? </li><li>Any other important observations.</li></ol>
<div> </div>
<div>Finally, we also need to evaporate Cesium from a compound like CsF or CsNO3. Any input on evaporating Cesium from these or any other preferred compounds would be very useful.</div>
<div>Thanks.</div>
<div> </div>
<div><font color="#1F497D">--</font></div>
<div><font color="#1F497D">Aamer Mahmood</font></div>
<div><font color="#1F497D">Senior Scientist</font></div>
<div><font color="#1F497D">Qatar Environment and Energy Research Institute, Qatar Foundation</font></div>
<div><font color="#1F497D">Doha, Qatar</font></div>
<div><font color="#1F497D">Tel: +974 44548132 (work)</font></div>
<div><font color="#1F497D"> </font></div>
<div><font color="#0000CC"><u><a href="http://www.qeeri.org.qa">www.qeeri.org.qa</a></u></font></div>
<div> </div>
<div> </div>
<div> </div>
</span></font>
<br clear="both">
This email message, including any attachments is intended solely for the addressee(s), and may contain information that is confidential or legally protected. Any use, disclosure, copying, printing or distribution of the information contained herein by persons other than the designated addressee is unauthorized and may be unlawful. If you believe that you have received this email in error, please notify the sender immediately and delete this email and any attachments from your system and discard any printout thereof. Qatar Foundation makes no warranty that this email is error- or virus-free .The views, opinions, conclusions, and other information expressed in this email are not necessarily endorsed by Qatar Foundation unless otherwise indicated by an authorized representative. As such, Qatar Foundation does not accept any liability for any emails and attachments that may violate the relevant applicable laws.<BR>
</body>
</html>