<html><head><meta http-equiv="content-type" content="text/html; charset=utf-8"></head><body dir="auto">Hi Rick,<div><br></div><div>We buy mask handling equipment from H-Square.  Is that who you are thinking of?</div><div><br></div><div><a href="http://www.h-square.com/A_Photomask_Handling.html">http://www.h-square.com/</a><br><br><div id="AppleMailSignature" dir="ltr">Jim Carroll</div><div dir="ltr">PhotomaskPORTAL</div><div dir="ltr"><br>On Jun 13, 2019, at 9:13 AM, Morrison, Richard H., Jr <<a href="mailto:rmorrison@draper.com">rmorrison@draper.com</a>> wrote:<br><br></div><blockquote type="cite"><div dir="ltr">

<meta http-equiv="Content-Type" content="text/html; charset=us-ascii">
<meta name="Generator" content="Microsoft Word 15 (filtered medium)">
<style><!--
/* Font Definitions */
@font-face
        {font-family:"Cambria Math";
        panose-1:2 4 5 3 5 4 6 3 2 4;}
@font-face
        {font-family:Calibri;
        panose-1:2 15 5 2 2 2 4 3 2 4;}
/* Style Definitions */
p.MsoNormal, li.MsoNormal, div.MsoNormal
        {margin:0in;
        margin-bottom:.0001pt;
        font-size:11.0pt;
        font-family:"Calibri",sans-serif;}
a:link, span.MsoHyperlink
        {mso-style-priority:99;
        color:#0563C1;
        text-decoration:underline;}
a:visited, span.MsoHyperlinkFollowed
        {mso-style-priority:99;
        color:#954F72;
        text-decoration:underline;}
span.EmailStyle17
        {mso-style-type:personal-compose;
        font-family:"Calibri",sans-serif;
        color:windowtext;}
.MsoChpDefault
        {mso-style-type:export-only;
        font-family:"Calibri",sans-serif;}
@page WordSection1
        {size:8.5in 11.0in;
        margin:1.0in 1.0in 1.0in 1.0in;}
div.WordSection1
        {page:WordSection1;}
--></style>


<div class="WordSection1">
<p class="MsoNormal">Hi Everyone,</p>
<p class="MsoNormal"> </p>
<p class="MsoNormal">For years we have been using Sensarray wafers to calibrate ovens and hot plates, the issue is they are silicon and break and at $7.5 k each it is costing me $$ I would rather spend on other things.</p>
<p class="MsoNormal"> </p>
<p class="MsoNormal">Do any of you use temperature calibration wafers made of metal, I used to get anodized Aluminum wafers for handler issues from H2Squared are they still around?</p>
<p class="MsoNormal"> </p>
<p class="MsoNormal">Thanks</p>
<p class="MsoNormal"> </p>
<p class="MsoNormal">Rick</p>
<p class="MsoNormal"> </p>
<p class="MsoNormal"> </p>
<p class="MsoNormal">Richard H. Morrison</p>
<p class="MsoNormal">Principal Member of the Technical Staff</p>
<p class="MsoNormal">Draper</p>
<p class="MsoNormal">555 Technology Square</p>
<p class="MsoNormal">Cambridge, MA</p>
<p class="MsoNormal">02139-3573</p>
<p class="MsoNormal"> </p>
<p class="MsoNormal">Work  617-258-3420</p>
<p class="MsoNormal">Cell  508-930-3461</p>
<p class="MsoNormal"><a href="http://www.draper.com">www.draper.com</a></p>
<p class="MsoNormal"> </p>
</div>
<hr>
Notice: This email and any attachments may contain proprietary (Draper non-public) and/or export-controlled information of Draper. If you are not the intended recipient of this email, please immediately notify the sender by replying to this email and immediately
 destroy all copies of this email.
<hr>


</div></blockquote><blockquote type="cite"><div dir="ltr"><span>_______________________________________________</span><br><span>labnetwork mailing list</span><br><span><a href="mailto:labnetwork@mtl.mit.edu">labnetwork@mtl.mit.edu</a></span><br><span><a href="https://mtl.mit.edu/mailman/listinfo.cgi/labnetwork">https://mtl.mit.edu/mailman/listinfo.cgi/labnetwork</a></span><br></div></blockquote></div></body></html>