Which brand of lamp you use ???<div><br></div><div>Regards <br><br><br><a href="https://yho.com/footer0">Sent from Yahoo Mail for iPhone</a><br><div>Mario Portillo, hbtusainc@yahoo.com</div><br><p class="yahoo-quoted-begin" style="font-size: 15px; color: #715FFA; padding-top: 15px; margin-top: 0">On Saturday, July 6, 2019, 6:09 AM, Matthias Pleil <mpleil@unm.edu> wrote:</p><blockquote class="iosymail"><div id="yiv0695126812"><div>
Hello Youry,<br clear="none">
<br clear="none">
1. We leave the lamp on all the time<br clear="none">
2. Change the lamp when it drops to about 2.2mW/cm^2, using 365nm meter<br clear="none">
3. Change about every six months or so.<br clear="none">
<br clear="none">
New lamp is about 3.2mW/cm^2<br clear="none">
<br clear="none">
Kind Regards,<br clear="none">
<br clear="none">
Matthias Pleil, Ph.D.<br clear="none">
Research Professor & Lecturer III of Mech. Eng - UNM<br clear="none">
UNM MTTC Cleanroom Manager<br clear="none">
PI - Southwest Center for Microsystems Education, Support Center for Microsystems Education<br clear="none">
scme-nm.org, scme-support.org<br clear="none">
<a dir="ltr" href="tel:(505)272-7157" x-apple-data-detectors="true" x-apple-data-detectors-type="telephone" x-apple-data-detectors-result="6">(505)272-7157</a><br clear="none">
<hr style="display:inline-block;width:98%;" tabindex="-1">
<div class="yiv0695126812yqt7324217437" id="yiv0695126812yqt54683"><div dir="ltr" id="yiv0695126812divRplyFwdMsg"><b>From:</b> labnetwork-bounces@mtl.mit.edu <labnetwork-bounces@mtl.mit.edu> on behalf of Youry Borisenkov <yb2471@columbia.edu><br clear="none">
<b>Sent:</b> Friday, July 5, 2019 9:58:44 AM<br clear="none">
<b>To:</b> labnetwork@mtl.mit.edu<br clear="none">
<b>Subject:</b> [labnetwork] MA6 lamp life
<div> </div>
</div>
<div>
<div dir="ltr">
<p class="yiv0695126812x_MsoNormal">HI Everyone,<u></u><u></u></p>
<p class="yiv0695126812x_MsoNormal"><u></u> <u></u></p>
<p class="yiv0695126812x_MsoNormal">I have 3 quick questions about your policy for changing the UV-lamp on the MA6 (Karl Suss) mask aligners. </p>
<p class="yiv0695126812x_MsoNormal">1. do you turn off the UV - power supply during nights and weekends? or just leave it on?</p>
<p class="yiv0695126812x_MsoNormal">2. do you change the UV lamp on a regular basis (after 1 month or so)? or you monitor it's power and have a lower limit before you decide to change it? or you just wait for it to fail and then change it?</p>
<p class="yiv0695126812x_MsoNormal">3. how often do you change the lamp?</p>
<p class="yiv0695126812x_MsoNormal"><br clear="none">
</p>
<p class="yiv0695126812x_MsoNormal">Thanks and Happy July 4<sup>th</sup><br clear="none">
</p>
<p class="yiv0695126812x_MsoNormal"><u></u></p>
<p class="yiv0695126812x_MsoNormal"><u></u>Youry</p>
<p class="yiv0695126812x_MsoNormal"><br clear="none">
</p>
<p class="yiv0695126812x_MsoNormal">P.S.</p>
<p class="yiv0695126812x_MsoNormal">You can use this template to reply):</p>
<table class="yiv0695126812x_gmail-MsoTableGrid" border="1" cellspacing="0" cellpadding="0" style="border-collapse:collapse;border:none;"><tbody><tr><td colspan="1" rowspan="1" valign="top" width="208" style="width:155.8pt;border:1pt solid windowtext;padding:0in 5.4pt;">
<p class="yiv0695126812x_gmail-MsoListParagraphCxSpFirst" style="margin:0in 0in 0.0001pt 0.5in;line-height:normal;font-size:11pt;font-family:Calibri, sans-serif;">
1-<span style="font-stretch:normal;font-size:7pt;line-height:normal;">
</span><span dir="LTR"></span>Off/On</p>
</td><td colspan="1" rowspan="1" valign="top" width="208" style="width:155.85pt;border-top:1pt solid windowtext;border-right:1pt solid windowtext;border-bottom:1pt solid windowtext;border-left:none;padding:0in 5.4pt;">
<p class="yiv0695126812x_gmail-MsoListParagraphCxSpMiddle" style="margin:0in 0in 0.0001pt 0.5in;line-height:normal;font-size:11pt;font-family:Calibri, sans-serif;">
2-<span style="font-stretch:normal;font-size:7pt;line-height:normal;">
</span><span dir="LTR"></span>Change every ___ / wait for the power to decrease by ___ % / wait for it to fail</p>
</td><td colspan="1" rowspan="1" valign="top" width="208" style="width:155.85pt;border-top:1pt solid windowtext;border-right:1pt solid windowtext;border-bottom:1pt solid windowtext;border-left:none;padding:0in 5.4pt;">
<p class="yiv0695126812x_gmail-MsoListParagraphCxSpLast" style="margin:0in 0in 0.0001pt 0.5in;line-height:normal;font-size:11pt;font-family:Calibri, sans-serif;">
3-<span style="font-stretch:normal;font-size:7pt;line-height:normal;">
</span><span dir="LTR"></span>Every ___ month</p>
</td></tr><tr><td colspan="1" rowspan="1" valign="top" width="208" style="width:155.8pt;border-right:1pt solid windowtext;border-bottom:1pt solid windowtext;border-left:1pt solid windowtext;border-top:none;padding:0in 5.4pt;">
<p class="yiv0695126812x_MsoNormal" style="margin:0in 0in 0.0001pt;line-height:normal;font-size:11pt;font-family:Calibri, sans-serif;">
</p>
</td><td colspan="1" rowspan="1" valign="top" width="208" style="width:155.85pt;border-top:none;border-left:none;border-bottom:1pt solid windowtext;border-right:1pt solid windowtext;padding:0in 5.4pt;">
<p class="yiv0695126812x_MsoNormal" style="margin:0in 0in 0.0001pt;line-height:normal;font-size:11pt;font-family:Calibri, sans-serif;">
</p>
</td><td colspan="1" rowspan="1" valign="top" width="208" style="width:155.85pt;border-top:none;border-left:none;border-bottom:1pt solid windowtext;border-right:1pt solid windowtext;padding:0in 5.4pt;">
<p class="yiv0695126812x_MsoNormal" style="margin:0in 0in 0.0001pt;line-height:normal;font-size:11pt;font-family:Calibri, sans-serif;">
</p>
</td></tr></tbody></table>
<p class="yiv0695126812x_MsoNormal"><br clear="none">
</p>
<p class="yiv0695126812x_MsoNormal">Youry Borisenkov, Ph.D.</p>
<p class="yiv0695126812x_MsoNormal">Process Engineer at CNI Shared Labs</p>
<p class="yiv0695126812x_MsoNormal"><u></u></p>
CEPSR/MC 8903<br clear="none">
530 west 120th st. NY<br clear="none">
NY 10027<br clear="none">
<p class="yiv0695126812x_MsoNormal">Work <a dir="ltr" href="tel:212-851-5688" x-apple-data-detectors="true" x-apple-data-detectors-type="telephone" x-apple-data-detectors-result="12">212-851-5688</a><u></u></p>
<p class="yiv0695126812x_MsoNormal">Cell <a dir="ltr" href="tel:646-592-1514" x-apple-data-detectors="true" x-apple-data-detectors-type="telephone" x-apple-data-detectors-result="13">646-592-1514</a></p>
</div>
</div></div>
</div></div><div class="yqt7324217437" id="yqt17174">_______________________________________________<br clear="none">labnetwork mailing list<br clear="none"><a shape="rect" ymailto="mailto:labnetwork@mtl.mit.edu" href="mailto:labnetwork@mtl.mit.edu">labnetwork@mtl.mit.edu</a><br clear="none"><a shape="rect" href="https://mtl.mit.edu/mailman/listinfo.cgi/labnetwork" target="_blank">https://mtl.mit.edu/mailman/listinfo.cgi/labnetwork</a><br clear="none"></div><blockquote></blockquote></blockquote></div>
</body></html>