<div dir="ltr"><div>I encourage evaluation of KJ Lesker</div><div>Bill Flounders</div><div>UC Berkeley<br></div><div><br></div><div><br></div><div>Contact:<br></div><div>
<table style="font-size:0px;color:rgb(31,73,125);font-style:normal;font-weight:700;white-space:nowrap" cellspacing="0" cellpadding="0" border="0"><tbody><tr style="font-size:16px"><td style="padding:0px;vertical-align:top;font-family:Arial" align="left">Pierre Hraiz<span style="font-family:remialcxesans;font-size:1px;color:rgb(255,255,255);line-height:1px"></span></td></tr><tr style="font-size:0px"><td style="padding:0px;vertical-align:top" align="left"><table style="font-size:0px;color:rgb(31,73,125);font-style:normal;font-weight:700;white-space:nowrap" cellspacing="0" cellpadding="0" border="0"><tbody><tr style="font-size:13px"><td style="vertical-align:top;font-family:Arial" align="left">Regional Sales Manager</td></tr><tr style="font-size:0px"><td style="vertical-align:top" align="left"><table style="width:100%;font-size:0px" cellspacing="0" cellpadding="0" border="0"><tbody><tr style="font-size:0px"><td style="vertical-align:top" align="left"><table style="width:100%;font-size:0px" cellspacing="0" cellpadding="0" border="0"><tbody><tr style="font-size:0px"><td style="vertical-align:top" align="left"><table style="width:100%;font-size:0px" cellspacing="0" cellpadding="0" border="0"><tbody><tr style="font-size:0px"><td style="vertical-align:top" align="left"><table style="width:100%;font-size:0px" cellspacing="0" cellpadding="0" border="0"><tbody><tr style="font-size:0px"><td style="vertical-align:top" align="left"><table style="font-size:0px;color:rgb(31,73,125);font-style:normal;font-weight:400;white-space:nowrap" cellspacing="0" cellpadding="0" border="0"><tbody><tr style="font-size:10.67px"><td style="padding:0px 0px 3px;vertical-align:top;font-family:Arial" align="left">Tel: <a href="tel:408-335-5779" id="gmail-m_3981579482084669043LPlnk689713" style="text-decoration:none;color:rgb(31,73,125)" target="_blank"><strong style="font-weight:400">408-335-5779</strong></a> (direct)</td></tr></tbody></table></td><td style="vertical-align:top" align="left"><table style="font-size:0px;color:rgb(31,73,125);font-style:normal;font-weight:400;white-space:nowrap" cellspacing="0" cellpadding="0" border="0"><tbody><tr style="font-size:10.67px"><td style="padding:0px 0px 3px 4px;vertical-align:top;font-family:Arial" align="left">| Cell: <a href="tel:(408)%20335-5779" id="gmail-m_3981579482084669043LPlnk689713" style="text-decoration:none;color:rgb(31,73,125)" target="_blank"><strong style="font-weight:400">(408) 335-5779</strong></a></td></tr></tbody></table></td></tr></tbody></table></td><td style="vertical-align:top" align="left"><table style="font-size:0px;color:rgb(31,73,125);font-style:normal;font-weight:400;white-space:nowrap" cellspacing="0" cellpadding="0" border="0"><tbody><tr style="font-size:10.67px"><td style="padding:0px 0px 3px 4px;vertical-align:top;font-family:Arial" align="left">| Email: <a href="mailto:pierreh@lesker.com" id="gmail-m_3981579482084669043LPlnk689713" style="text-decoration:none;color:rgb(31,73,125)" target="_blank"><strong style="font-weight:400">pierreh@lesker.com</strong></a> </td></tr></tbody></table></td></tr></tbody></table></td></tr><tr style="font-size:0px"><td style="vertical-align:top" align="left"><table style="font-size:0px;line-height:normal" cellspacing="0" cellpadding="0" border="0"><tbody><tr style="font-size:0px"><td style="padding:0px 0px 2px;vertical-align:top" align="left"><br></td></tr></tbody></table></td></tr></tbody></table></td></tr></tbody></table></td></tr></tbody></table></td></tr></tbody></table>
</div></div><br><div class="gmail_quote"><div dir="ltr" class="gmail_attr">On Fri, Jul 17, 2020 at 5:49 AM Guido Janssen - 3ME <<a href="mailto:G.C.A.M.Janssen@tudelft.nl">G.C.A.M.Janssen@tudelft.nl</a>> wrote:<br></div><blockquote class="gmail_quote" style="margin:0px 0px 0px 0.8ex;border-left:1px solid rgb(204,204,204);padding-left:1ex">Dear colleagues<br>
<br>
Here in Delft we are in the proces of replacing our 16 years old AJA sputter tool, used for proces development and materials science studies.<br>
We’re looking for a system with three 2” targets in sputter down configuration able to handle small samples as well as 100 mm wafers. DC and RF, heated substrate holder with sample bias option, turbo pumped and equiped with a load lock. <br>
Do you know of any supplier other than AJA that offers such a system?<br>
<br>
Sincerely<br>
Guido Janssen<br>
TU Delft<br>
<a href="mailto:g.c.a.m.janssen@tudelft.nl" target="_blank">g.c.a.m.janssen@tudelft.nl</a><br>
_______________________________________________<br>
labnetwork mailing list<br>
<a href="mailto:labnetwork@mtl.mit.edu" target="_blank">labnetwork@mtl.mit.edu</a><br>
<a href="https://mtl.mit.edu/mailman/listinfo.cgi/labnetwork" rel="noreferrer" target="_blank">https://mtl.mit.edu/mailman/listinfo.cgi/labnetwork</a><br>