<div dir="ltr">A faculty member installed an Easytube CVD system in our microfab for producing CNTs, with the plan to produce spinable CNT fibers. They are just using out electron beam for producing the catalyst substrates - currently electron beam of 10 nm Al that they then oxidize and then 2 nm of Fe - all on 300 nm of thermal SiO2/Si. They did investigate sputtering Al2O3 instead. So far they have produced CNTs, but have not found the recipe that will produce long spinable fibers. They are using a H2 and C2H4 gas mixture and grow around 750degC. <div><br></div><div>I was wanting to see if anyone runs a user system that they guarantee spinable CNTs. If so I was wanting to talk, offline, about tuning the process and possibly getting some of their catalyst substrates to compare. I have been letting the student work on the recipe development as I have other issues to worry about and it is their system.</div><div><br></div><div>Chito Kendrick </div><div><div><div><br></div>-- <br><div dir="ltr" class="gmail_signature" data-smartmail="gmail_signature"><div dir="ltr"><div><div dir="ltr"><span><font color="#888888"><a href="https://sites.google.com/site/chitokendrickphd/" target="_blank">Chito
Kendrick Ph.D.</a><br>
<br>Managing Director of the Microfabrication Facility<br>
Research Assistant Professor<br>
Electrical and Computer Engineering<br>
Michigan Technological University<br>
Room 436 M&M Building<br>
1400 Townsend Dr.<br>
Houghton, Michigan 49931-1295<br>
<br>
<a href="tel:814-308-4255" value="+18143084255" target="_blank">814-308-4255</a></font></span></div></div></div></div></div></div></div>