<div dir="ltr">Hi,<div><br></div><div>We can help you at University of Illinois.We can do AlOx, HfOx and SiOx. </div><div>Sending your samples for us to do deposition is probably the easiest and fastest option. </div><div><br></div><div>You can contact me directly at <a href="mailto:echow@illinois.edu">echow@illinois.edu</a></div><div><br></div><div>Edmond</div></div><br><div class="gmail_quote"><div dir="ltr" class="gmail_attr">On Mon, Aug 10, 2020 at 11:13 AM Shepard, Jeremiah J <<a href="mailto:jshepar@purdue.edu">jshepar@purdue.edu</a>> wrote:<br></div><blockquote class="gmail_quote" style="margin:0px 0px 0px 0.8ex;border-left:1px solid rgb(204,204,204);padding-left:1ex">
<div dir="ltr">
<div style="color:rgb(0,0,0);font-family:Calibri,Arial,Helvetica,sans-serif;font-size:12pt">
<span>All,</span></div>
<div style="color:rgb(0,0,0);font-family:Calibri,Arial,Helvetica,sans-serif;font-size:12pt">
<span>Good morning! I am an engineer with Purdue's Birck Nanotechnology fab. Our ALD system has went down and will be down for several weeks. I am looking for alternatives for our researchers to use until our system comes back online. We are located in
West Lafayette, Indiana and options would need to be within a few hours driving distance of our location, or provide the service through mail. </span></div>
<div style="color:rgb(0,0,0);font-family:Calibri,Arial,Helvetica,sans-serif;font-size:12pt">
<span><br>
</span></div>
<div style="color:rgb(0,0,0);font-family:Calibri,Arial,Helvetica,sans-serif;font-size:12pt">
<span>Our system is equipped with AlOx, HfOx, and SiOx. The majority of our users are growing AlOx and HfOx. We have many users interested in low temp growths at 90 to 110 C and we have a limit of 50 nm film thickness. We also have many users growing at
more traditional 200 C temps. I would expect work coming from our fab to fall within these parameters.</span></div>
<div style="color:rgb(0,0,0);font-family:Calibri,Arial,Helvetica,sans-serif;font-size:12pt">
<span><br>
</span></div>
<div style="color:rgb(0,0,0);font-family:Calibri,Arial,Helvetica,sans-serif;font-size:12pt">
<span>Any leads would be greatly appreciated!</span></div>
<div style="color:rgb(0,0,0);font-family:Calibri,Arial,Helvetica,sans-serif;font-size:12pt">
<span><br>
</span></div>
<div style="color:rgb(0,0,0);font-family:Calibri,Arial,Helvetica,sans-serif;font-size:12pt">
<span>Thank you,</span></div>
<div style="color:rgb(0,0,0);font-family:Calibri,Arial,Helvetica,sans-serif;font-size:12pt">
<span>Jerry Shepard</span></div>
<div style="color:rgb(0,0,0);font-family:Calibri,Arial,Helvetica,sans-serif;font-size:12pt">
<span><br>
</span></div>
</div>
_______________________________________________<br>
labnetwork mailing list<br>
<a href="mailto:labnetwork@mtl.mit.edu" target="_blank">labnetwork@mtl.mit.edu</a><br>
<a href="https://mtl.mit.edu/mailman/listinfo.cgi/labnetwork" rel="noreferrer" target="_blank">https://mtl.mit.edu/mailman/listinfo.cgi/labnetwork</a><br>
</blockquote></div><br clear="all"><div><br></div>-- <br><div dir="ltr" class="gmail_signature">Edmond Chow</div>