Hi Jerry, <br>
</div>
<div style="font-family: Calibri, Arial, Helvetica, sans-serif; font-size: 12pt; color: rgb(0, 0, 0);">
   Our Beneq system is up and running at U of Louisville. Currently our precursors are ZnO, Al2O3, and TiO2. If your users need a lot of depositions with another material, we would be happy to consider stocking it. 
<a href="https://louisville.edu/micronano" id="LPlnkOWALinkPreview_0">https://louisville.edu/micronano</a>
<br>
</div>
<div class="_Entity _EType_OWALinkPreview _EId_OWALinkPreview_0 _EReadonly_1">
<div id="LPBorder_GTaHR0cHM6Ly9sb3Vpc3ZpbGxlLmVkdS9taWNyb25hbm8." class="LPBorder772576" style="width: 100%; margin-top: 16px; margin-bottom: 16px; position: relative; max-width: 800px; min-width: 424px;">
<table id="LPContainer772576" role="presentation" style="padding: 12px 36px 12px 12px; width: 100%; border-width: 1px; border-style: solid; border-color: rgb(200, 200, 200); border-radius: 2px;">
<tbody>
<tr style="border-spacing: 0px;" valign="top">
<td style="width: 100%;">
<div id="LPTitle772576" style="font-size: 21px; font-weight: 300; margin-right: 8px; font-family: "wf_segoe-ui_light", "Segoe UI Light", "Segoe WP Light", "Segoe UI", "Segoe WP", Tahoma, Arial, sans-serif; margin-bottom: 12px;">
<a target="_blank" id="LPUrlAnchor772576" href="https://louisville.edu/micronano" style="text-decoration: none; color:var(--themePrimary);">Welcome to MNTC — Micro/Nano Technology Center</a></div>
<div id="LPDescription772576" style="font-size: 14px; max-height: 100px; color: rgb(102, 102, 102); font-family: "wf_segoe-ui_normal", "Segoe UI", "Segoe WP", Tahoma, Arial, sans-serif; margin-bottom: 12px; margin-right: 8px; overflow: hidden;">
The MNTC is OPEN. A new entry protocol has been implemented for both the cleanroom and the Huson Lab. Contact us before entering either lab, so we may train you on the new protocol.</div>
<div id="LPMetadata772576" style="font-size: 14px; font-weight: 400; color: rgb(166, 166, 166); font-family: "wf_segoe-ui_normal", "Segoe UI", "Segoe WP", Tahoma, Arial, sans-serif;">
louisville.edu</div>
</td>
</tr>
</tbody>
</table>
</div>
</div>
<br>
<div style="font-family: Calibri, Arial, Helvetica, sans-serif; font-size: 12pt; color: rgb(0, 0, 0);">
<br>
</div>
<div style="font-family: Calibri, Arial, Helvetica, sans-serif; font-size: 12pt; color: rgb(0, 0, 0);">
Regards, <br>
</div>
<div style="font-family: Calibri, Arial, Helvetica, sans-serif; font-size: 12pt; color: rgb(0, 0, 0);">
   Michael   <br>
</div>
<div id="appendonsend"></div>
<hr style="display:inline-block;width:98%" tabindex="-1">
<div id="divRplyFwdMsg" dir="ltr"><font face="Calibri, sans-serif" style="font-size:11pt" color="#000000"><b>From:</b> labnetwork-bounces@mtl.mit.edu <labnetwork-bounces@mtl.mit.edu> on behalf of Shepard, Jeremiah J <jshepar@purdue.edu><br>
<b>Sent:</b> Monday, August 10, 2020 9:04 AM<br>
<b>To:</b> labnetwork@mtl.mit.edu <labnetwork@mtl.mit.edu><br>
<b>Subject:</b> [labnetwork] ALD availability in the midwest</font>
<div> </div>
</div>
<style type="text/css" style="display:none">
<!--
p
        {margin-top:0;
        margin-bottom:0}
-->
</style>
<div dir="ltr">
<p class="x_MsoNormal" style="line-height:12.0pt; background:#FF4D4D"><b><span style="font-size:10.0pt; color:black">CAUTION:</span></b><span style="font-size:10.0pt; color:black"> This email originated from outside of our organization. Do not click links,
 open attachments, or respond unless you recognize the sender's email address and know the contents are safe.</span></p>
<div></div>
<div>
<div style="color:rgb(0,0,0); font-family:Calibri,Arial,Helvetica,sans-serif; font-size:12pt">
<span>All,</span></div>
<div style="color:rgb(0,0,0); font-family:Calibri,Arial,Helvetica,sans-serif; font-size:12pt">
<span>Good morning!  I am an engineer with Purdue's Birck Nanotechnology fab.  Our ALD system has went down and will be down for several weeks.  I am looking for alternatives for our researchers to use until our system comes back online.  We are located in
 West Lafayette, Indiana and options would need to be within a few hours driving distance of our location, or provide the service through mail.  </span></div>
<div style="color:rgb(0,0,0); font-family:Calibri,Arial,Helvetica,sans-serif; font-size:12pt">
<span><br>
</span></div>
<div style="color:rgb(0,0,0); font-family:Calibri,Arial,Helvetica,sans-serif; font-size:12pt">
<span>Our system is equipped with AlOx, HfOx,  and SiOx.  The majority of our users are growing AlOx and HfOx.  We have many users interested in low temp growths at 90 to 110 C and we have a limit of 50 nm film thickness.  We also have many users growing at
 more traditional 200 C temps.  I would expect work coming from our fab to fall within these parameters.</span></div>
<div style="color:rgb(0,0,0); font-family:Calibri,Arial,Helvetica,sans-serif; font-size:12pt">
<span><br>
</span></div>
<div style="color:rgb(0,0,0); font-family:Calibri,Arial,Helvetica,sans-serif; font-size:12pt">
<span>Any leads would be greatly appreciated!</span></div>
<div style="color:rgb(0,0,0); font-family:Calibri,Arial,Helvetica,sans-serif; font-size:12pt">
<span><br>
</span></div>
<div style="color:rgb(0,0,0); font-family:Calibri,Arial,Helvetica,sans-serif; font-size:12pt">
<span>Thank you,</span></div>
<div style="color:rgb(0,0,0); font-family:Calibri,Arial,Helvetica,sans-serif; font-size:12pt">
<span>Jerry Shepard</span></div>
<div style="color:rgb(0,0,0); font-family:Calibri,Arial,Helvetica,sans-serif; font-size:12pt">
<span><br>
</span></div>
</div>
</div>
</body>
</html>