                        An alternative source for HSQ is <br>
                        <pre><a href="http://discheminc.com" target="_blank">discheminc.com</a> </pre>

<div>XR1541 is Dow's brand name for HSQ.</div><div>Dischem's product is pretty much a drop-in replacement, except for having to bake it at 120C after spinning.</div><div><br></div><div>EMResist in the UK also sells HSQ, but I have not tried it.</div><div><br></div><div><br></div><div><div><div dir="ltr" class="gmail_signature" data-smartmail="gmail_signature"><div dir="ltr">--------------------------------<div><font size="1">Michael Rooks</font></div><div><font size="1"><a href="http://nano.yale.edu" target="_blank">nano.yale.edu</a></font> </div></div></div></div><br></div></div><br><div class="gmail_quote"><div dir="ltr" class="gmail_attr">On Tue, Sep 8, 2020 at 7:40 PM Franklin Monzon <<a href="mailto:fm@fmconsultingresearch.com">fm@fmconsultingresearch.com</a>> wrote:<br></div><blockquote class="gmail_quote" style="margin:0px 0px 0px 0.8ex;border-left:1px solid rgb(204,204,204);padding-left:1ex"><div>Hi All,</div>
<div> </div>
<div>We at HRL are having enormous difficulty with procurement of ebeam resist from Dow, and I wonder if anyone else is having this problem. Specifically, we are trying to acquire XR-1541. We use 2%, 4%, and 6% formulations but are having special problems with 2%.</div>
<div> </div>
<div>Lead times have increased generally in 2020 (perhaps for some good reasons!), but the distributors we work with now cannot even get a firm timeline from Dow. We told them we are willing to order larger quantities than usual but have been informed that that won't help.</div>
<div> </div>
<div>The shortage is starting to cause delays on key government programs, so I'd very much appreciate any insight from this group.</div>
<div> </div>
<div>Thanks for your advice!</div>
<div>FM</div>
<div>*********************************</div>
<div>Franklin Monzon</div>
<div>Director, Microfabrication Technology Laboratory</div>
<div>HRL Laboratories</div>
<div> </div>
<div> </div>
_______________________________________________<br>
labnetwork mailing list<br>
<a href="mailto:labnetwork@mtl.mit.edu" target="_blank">labnetwork@mtl.mit.edu</a><br>
<a href="https://mtl.mit.edu/mailman/listinfo.cgi/labnetwork" rel="noreferrer" target="_blank">https://mtl.mit.edu/mailman/listinfo.cgi/labnetwork</a><br>
</blockquote></div>