Hi All,
<div class=""><br class="">
</div>
<div class="">I’m looking for HSQ alternatives since it’s expensive, has a 14 week lead time and comes in 250mL bottle. We waste most of the bottle due to it’s 6 months shelf life. Although we had some bottles still good after 2 years at 5C, it’s just a huge
gamble after a year. We tried LN2 freezing, but it takes too much effort.</div>
<div class=""><br class="">
</div>
<div class="">I’ve attached a table of the cost per mL for the alternatives I found assuming you want 100nm thick. The AQM and EMResist are in powder form and advertise 1 year powder shelf life and 3 months mixture shelf life. They can distribute the powder
into many small bottles. </div>
<div class=""><br class="">
</div>
<div class="">Particularly interesting is the Medusa 82 which has the lowest cost and advertises better shelf life. Does anyone have experience with these HSQ alternatives?</div>
<div class=""><br class="">
</div>
<div class=""><img apple-inline="yes" id="B22AB60B-4D51-4545-A7EB-6C2B9D076D07" src="cid:EA246686-78D1-44AC-9192-C364E1E8651D@serc.dhcp.e.uh.edu" class=""></div>
<div class=""><br class="">
</div>
<div class="">Thanks,<br class="">
<div class="">
<div dir="auto" style="caret-color: rgb(0, 0, 0); color: rgb(0, 0, 0); letter-spacing: normal; text-align: start; text-indent: 0px; text-transform: none; white-space: normal; word-spacing: 0px; -webkit-text-stroke-width: 0px; text-decoration: none; word-wrap: break-word; -webkit-nbsp-mode: space; line-break: after-white-space;" class="">
Long</div>