<div dir="ltr">We have a lab user who is interested in sputtering vanadium dioxide. I realize this has been asked before without an answer, but I thought I'd try again. Does anybody have a VO2 process running and would be willing to do some depositions for us?<div>Barring that, does anybody have any tips or successes with reactively sputtering VO2?</div><div><br></div><div>Thanks for the help.<br clear="all"><div><br></div>-- <br><div dir="ltr" class="gmail_signature" data-smartmail="gmail_signature"><div dir="ltr"><div dir="ltr"><div dir="ltr"><div dir="ltr"><div dir="ltr">Darick Baker, PhD<br>Business Outreach and Customer Development<br>New User Orientation<br>Research Engineer - Deposition<br>Washington Nanofabrication Facility (WNF)<br>University of Washington<br>Fluke Hall 115, Box 352143<br>Desk: 206.221.8265 Cell: 206.395.4049<br><a href="mailto:fab-support@wnf.uw.edu">fab-support@wnf.uw.edu</a><br><a href="https://www.wnf.washington.edu/">https://www.wnf.washington.edu/</a><br>Pronouns: he/him<br></div></div></div></div></div></div></div></div>