    We have a pulsed laser deposition (PLD) system here at UD which is
    mostly used for Vanadium oxide deposition. PLD is more suited for
    depositing oxides than sputtering.<br>
    <br>
    Please send me a note if you would like to discuss.<br>
    <br>
    Cheers,<br>
    <br>
    Iulian<br>
    <br>
    <br>
    <pre class="moz-signature" cols="72">iulian Codreanu, Ph.D.
Director, Nanofabrication Facility
University of Delaware
Harker ISE Lab, Room 163
221 Academy Street
Newark, DE 19716
302-831-2784
<a class="moz-txt-link-freetext" href="http://udnf.udel.edu">http://udnf.udel.edu</a></pre>
    <div class="moz-cite-prefix">On 6/9/2021 7:43 PM, Darick Baker
      wrote:<br>
    </div>
    <blockquote type="cite"
cite="mid:CAJTeEcrZjvbtgcyFpOC99Wx2_M7_gQ=yGh1OKZ17k4Cf-y6f6Q@mail.gmail.com">
      <meta http-equiv="content-type" content="text/html; charset=UTF-8">
      <div dir="ltr">We have a lab user who is interested in sputtering
        vanadium dioxide. I realize this has been asked before without
        an answer, but I thought I'd try again. Does anybody have a VO2
        process running and would be willing to do some depositions for
        us?
        <div>Barring that, does anybody have any tips or successes with
          reactively sputtering VO2?</div>
        <div><br>
        </div>
        <div>Thanks for the help.<br clear="all">
          <div><br>
          </div>
          -- <br>
          <div dir="ltr" class="gmail_signature"
            data-smartmail="gmail_signature">
            <div dir="ltr">
              <div dir="ltr">
                <div dir="ltr">
                  <div dir="ltr">
                    <div dir="ltr">Darick Baker, PhD<br>
                      Business Outreach and Customer Development<br>
                      New User Orientation<br>
                      Research Engineer - Deposition<br>
                      Washington Nanofabrication Facility (WNF)<br>
                      University of Washington<br>
                      Fluke Hall 115, Box 352143<br>
                      Desk: 206.221.8265 Cell: 206.395.4049<br>
                      <a href="mailto:fab-support@wnf.uw.edu"
                        moz-do-not-send="true">fab-support@wnf.uw.edu</a><br>
                      <a href="https://www.wnf.washington.edu/"
                        moz-do-not-send="true">https://www.wnf.washington.edu/</a><br>
                      Pronouns: he/him<br>
                    </div>
                  </div>
                </div>
              </div>
            </div>
          </div>
        </div>
      </div>
      <br>
      <fieldset class="mimeAttachmentHeader"></fieldset>
      <pre class="moz-quote-pre" wrap="">_______________________________________________
labnetwork mailing list
<a class="moz-txt-link-abbreviated" href="mailto:labnetwork@mtl.mit.edu">labnetwork@mtl.mit.edu</a>
<a class="moz-txt-link-freetext" href="https://mtl.mit.edu/mailman/listinfo.cgi/labnetwork">https://mtl.mit.edu/mailman/listinfo.cgi/labnetwork</a>
</pre>
    </blockquote>
    <br>
  </body>
</html>