<div>We have an old Branson S3100 plasma asher in the LSU nanofab. We believe the matching network is in need of repair. The power supply is stable when connected to a dummy load but gives unstable power output when connected to the matching network/chamber.</div>
<div dir="auto" style="text-align: left;"><br>
</div>
<div dir="auto" style="text-align: left;">Does anyone on the list know of a reliable 3rd party that works on these old tools? Thanks!</div>