<div>I assume you are coating your carrier wafer - too much exposed silicon can be a problem. Always make sure you develop your process for a fixed amount of exposed silicon and try to maintain it.</div>
<div id="ms-outlook-mobile-signature">
<div><br>
</div>
Get <a href="https://aka.ms/o0ukef">Outlook for iOS</a></div>
</div>
</div>
<hr style="display:inline-block;width:98%" tabindex="-1">
<div id="divRplyFwdMsg" dir="ltr"><font face="Calibri, sans-serif" style="font-size:11pt" color="#000000"><b>From:</b> labnetwork <labnetwork-bounces@mtl.mit.edu> on behalf of Shepard, Jeremiah J <jshepar@purdue.edu><br>
<b>Sent:</b> Wednesday, July 21, 2021 8:43:32 AM<br>
<b>To:</b> labnetwork@mtl.mit.edu <labnetwork@mtl.mit.edu><br>
<b>Subject:</b> [labnetwork] ICP STS ASE Issue</font>
<div> </div>
</div>
<style type="text/css" style="display:none">
<!--
p
{margin-top:0;
margin-bottom:0}
-->
</style>
<div dir="ltr">
<div style="font-family:Calibri,Arial,Helvetica,sans-serif; font-size:12pt; color:rgb(0,0,0)">
I am having some trouble determining what this issue is? We have found a bad capacitor in the matching network, and replaced that, thought all was good but now we face this issue. </div>
<div style="font-family:Calibri,Arial,Helvetica,sans-serif; font-size:12pt; color:rgb(0,0,0)">
<br>
</div>
<div style="font-family:Calibri,Arial,Helvetica,sans-serif; font-size:12pt; color:rgb(0,0,0)">
Now I am having trouble with grass formation on student sample. Anyone know where to look for this kind of thing? Is it just sample recipe or something else perhaps? Any thoughts are appreciated! Also unsure of what's going on with the carrier wafer around
the sample...?</div>
<div style="font-family:Calibri,Arial,Helvetica,sans-serif; font-size:12pt; color:rgb(0,0,0)">
<br>
</div>
<div style="font-family:Calibri,Arial,Helvetica,sans-serif; font-size:12pt; color:rgb(0,0,0)">
Thanks,</div>
<div style="font-family:Calibri,Arial,Helvetica,sans-serif; font-size:12pt; color:rgb(0,0,0)">
Jerry Shepard</div>
<div style="font-family:Calibri,Arial,Helvetica,sans-serif; font-size:12pt; color:rgb(0,0,0)">
<br>
</div>
<div style="font-family:Calibri,Arial,Helvetica,sans-serif; font-size:12pt; color:rgb(0,0,0)">
<img size="747979" data-outlook-trace="F:1|T:1" src="cid:b5ebd4e6-f9a5-41ac-91e8-fb784f88dacc" style="max-width:100%"><br>
</div>
</div>
</body>
</html>